ASTM A671 ERW Steel Tiyo

Kabòn Steel ASTM A671 EFW Dwat Couture soude tiyo fèt pou aplikasyon pou kote ranje tanperati a se ant anbyen ak kriyojenik.ASTM A671 Kabòn Steel tiyo se te fè soti nan plak kalite veso presyon.
Voye rechèch
Pwodwi Entwodiksyon

ASTM A671 ERW Tiyo Supplier-GNEE

Se tiyo ASTM A671 EFW prensipalman itilize nan lwil oliv ak gaz ak pwosesis chimik ak endistri jenerasyon pouvwa. Tiyo sa yo itilize tou nan pwojè enfrastrikti tankou sistèm dlo ak egou. Anplis de sa, yo te itilize nan konstriksyon an nan pon, bilding ak lòt estrikti ki mande pou durability ak rezistans fwotman.

 

Espesifikasyon estanda A671
Kòd ak Estanda

ANSI, ASME, ASTM, API, SAE, BS, AGA, AWWA, ISO, DIN

Dimansyon ASME / ANSI B36.10 / 19
Gwosè estanda 1/2" NB pou 36" NB (EFW)
Epesè miray la 3-12mm
Orè tiyo yo SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Pwodui teknik EFW / ERW / soude / fabrike
Fòm ki disponib Wonn, mwatye wonn, kare, rektangilè oswa fòm Custom
Longè 3 a Max18 mèt oswa koutim
Fen tiyo Bizote Fen, Plain Fen, Treaded
Sètifika tès EN 10204 3.1 B

 

A671 Tiyo Chimik konpatibilite

A671 Klas Konpozisyon chimik
C Si Mn P S Ti
             
-/A45 -/0.17 - 0.98 0.035 0.035 -
-/A50 -/0.22 -
CA55 / A55 0.28 -
-/B55 -/0.20 0.13
~0.45
CB60 / B60 0.24
CB65 / B65 0.28
CB70 / C70 0.31 1.30
-/C55 -/0.18 0.55
~0.98
CC60/ C60 0.21
CC65 / C65 0.24 0.79
~1.30
CC70 / C70 0.27

 

ASTM A671 EFW soude tiyo mekanik pwopwiyete résistance fòs

Klas Fòs Sede (N/mm2) Pwopriyete Tensile (N/mm2) elongasyon (%) Fòs rupture pwen soude (N/mm2)
-/A45 -/165 -/310~450 -/30 -/310~450
-/A50 -/185 -/345~485 -/28 -/345~485
CA55 / A55 205 380~515 27 380~515
-/B55 -/205 -/380~515 -/27 -/380~515
CB60 / B60 220 415~550 25 415~550
CB65 / B65 240 450~585 23 450~585
CB70 / C70 260 485~620 21 485~620
-/C55 -/205 -/380~515 -/27 -/380~515
CC60/ C60 220 415~550 25 415~550
CC65 / C65 240 450~585 23 450~585
CC70 / C70 260 485~620 21 485~620

 