P235GH, P265GH, P235TR1 ERW Tib
EN 10216 Welded Pipe Supplier-GNEE
EN 10216-1 P235tr1 trete an akò ak estanda nasyonal ak entènasyonal yo. Eleman nan klas sa a yo te itilize nan aplikasyon pou wo-tanperati tankou lwil oliv ak gaz, ekipman chofaj, echanjeur chalè, elatriye P265gh Tc1 materyèl ki fèt yo gen ekselan pwopriyete mekanik. Fòs rupture nan materyèl la varye ant 360 ak 500mpa. Yo gen yon fòs sede minimòm de 235mpa epi yo ka long pa 25%. P235GH se yon asye espesifye nan Ewòp pou veso presyon, chodyèr ak echanjeur chalè. Konpozisyon sa a asye fè li depreferans adapte nan aplikasyon pou travay wo-tanperati ak materyèl la itilize pa manifaktirè nan tout lwil oliv, gaz ak endistri pétrochimique.
Estanda: EN10216-1, EN10216 -2
Dyamèt (OD): 21,3 mm-610,0 mm
Epesè miray (WT): 2.0 mm-60.0 mm
Longè: 5.8-11.8m
Tretman kondisyon:+N
Tablo tolerans nan EN 10216-1 Tiyo asye soude
| Egzekisyon | Gwosè Range | OD Tolerans | Mi tolerans |
|---|---|---|---|
| Cho-woule Tib | OD – 80 milimeterOD > 80 milimeterWall < 12 milimeterWall - 12 milimèt | ± {{0}}.4 milimèt± 0.5% OD | ± 0.7 milimèt± (5 % x epesè miray + 0.1 milimèt |
| Cho-woule tib kale | Tout gwosèMi < 12 milimètMi - 12 milimèt | + 0.25/- 0 milimèt | ± 0.8 milimèt± (5 % x epesè miray + 0.2 milimèt) |
| Fwad Travay tib woule frèt oswa trase frèt | OD < 40 milimeterOD 40 - 80 milimeterOD > 80 Epesè miray la< 6 milimeter Wall Thickness6 - 8 milimeter Wall Thickness > 8 | + 0.30/- 0 milimèt*+ 0.35/- 0 milimèt*+ 0.40/- 0 milimèt* | ± {{0}}.30 milimèt± 0.35 milimèt± 0.40 milimèt |
ERW Tib konpozisyon chimik:
| Steel Klas |
C |
Si |
Mn |
P |
S |
Kr |
Mo |
Ni |
Al |
Cu |
Nb |
Ti |
V |
Cr+Cu+ Mo+Ni |
|
| Non Steel | Nimewo Steel | max | max | max | max | max | max | max | max | min | max | max | max | max | max |
| P195TR1 | 1.0107 | 0.13 | 0.35 | 0.70 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 | - | 0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
| P195TR2 | 1.0108 | 0.13 | 0.35 | 0.70 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 | 0.02 | 0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
| P235TR1 | 1.0254 | 0.16 | 0.35 | 1.20 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 | - | 0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
| P235TR2 | 1.0255 | 0.16 | 0.35 | 1.20 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 | 0.02 | 0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
| P265TR1 | 1.0258 | 0.20 | 0.40 | 1.40 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 |
- |
0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
| P265TR2 | 1.0259 | 0.20 | 0.40 | 1.40 | 0.025 | 0.020 | 0.30 | 0.08 | 0.30 | 0.02 | 0.30 | 0.010 | 0.04 | 0.02 | 0.70 |
EN 10216 ERW Steel Tib Detay


Baj popilè: p235gh, p265gh, p235tr1 erw tib, Lachin p235gh, p265gh, p235tr1 erw tib manifaktirè, founisè