API 5L ERW PSL 2 tiyo
API 5L PLS2 estanda apwopriye pou transpòte gaz, dlo ak lwil oliv nan endistri lwil oliv ak gaz natirèl.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon
Estanda API 5L a gen règleman detaye sou klas asye ak klas tiyo. Se klas asye divize an de klas: PLS1 ak PLS2. Chak nivo divize an plizyè nivo: A25, A, B, X42, X46, X52, X56, X60, X65, X70, X80, X100, ak X120.
API 5L PLS2 Spesifikasyon
| Ranje gwosè OD: |
ERW:0.375" jiska 30" SMLS:0.840" jiska 26" |
|---|---|
| Epesè miray API 5L: | ERW:0.120" jiska 1.000" HF:0.120" jiska 1.000" DSAW/SAWL:0.250" jiska 6.000" SMLS:0.250" jiska 2.500" HSAW:0.250" jiska 1.000" |
| Longè: | Single Random Double Random Custom (jiska 300') |
| Fini sifas: | Bare, lwil oliv, Mill vèni, Galv, FBE, FBE Doub, 3LPE, 3LPP, goudwon chabon, kouch konkrè ak vlope tep. Plizyè pwojè asye tiyo ekstèn kouch yo aktyèlman aplike pa konpayi nou an ki gen ladan yon sèl-kouch / doub-kouch FBE, 2PE, 3PE, 3PP ak lòt kouch anti-korozyon ak estanda yo fè tankou DIN30670, DIN30671, DIN30678, CAN / CSA-Z245. .21-M92,SY/T4013-2002 ak SY/T0315-97 elatriye. |
| Fini fini: | Bizote, Koupe kare, Threaded & Makonnen. |
| Sèvis adisyonèl: | Entèn kouch |
| Kabòn Steel Tiyo & Tib Creole | API 5L, API -2B, CSA Z245, ASTM A53, A106, ASTM A252, AS 1163, IPS 190 elatriye ASTM A53, ASTM A106, ASTM A500/501-98, ASTM A519-98, JIS G3441-1994, JIS G3444-1994, BS EN 10210-1, GB{{ 8}}, ASTM A179, ASTM A106, JIS G3454, GB/T8163-1999, ASTM A53-98, JIS G3452-1998, JIS G3454-1998, ASTM A106, DIN 1629-1984, API 5D, GB9948-1988 |
API 5L soude tiyo dimansyon
| NB | DN | OD (pous) | Orè | ||||||||||
| SCH 5 | SCH 10 | SCH 20 | SCH 30 | SCH 40 | SCH 60 | SCH 80 | SCH 100 | SCH 120 | SCH 160 | ||||
| 3/4" | 20 | 1.05 | 0.065 | 0.11 | x | 0.095 | 0.113 | x | x | 0.17 | x | 0.219 | |
| 1" | 25 | 1.315 | 0.065 | 0.11 | x | 0.114 | 0.133 | x | x | 0.2 | x | 0.25 | |
| 1.1/2" | 40 | 1.9 | 0.065 | 0.11 | x | 0.125 | 0.145 | x | x | 0.225 | x | 0.281 | |
| 2" | 50 | 2.375 | 0.065 | 0.12 | x | x | 0.154 | x | x | 0.25 | x | 0.344 | |
| 2.1/2" | 65 | 2.875 | 0.083 | 0.12 | x | x | 0.203 | x | x | 0.3 | x | 0.375 | |
| 3" | 80 | 3.5 | 0.083 | 0.12 | x | x | 0.216 | x | x | 0.35 | x | 0.438 | |
| 4" | 100 | 4.5 | 0.083 | 0.12 | x | x | 0.237 | x | x | 0.437 | x | 0.531 | |
| 5" | 125 | 5.563 | 0.109 | 0.12 | x | x | 0.258 | x | x | 0.5 | x | 0.625 | |
| 6" | 150 | 6.625 | 0.109 | 0.13 | x | x | 0.28 | x | x | 0.562 | x | 0.719 | |
| 8" | 200 | 8.625 | 0.109 | 0.15 | 0.25 | 0.277 | 0.322 | 0.406 | 0.593 | 0.718 | 0.812 | 0.906 | |
| 10" | 250 | 10.75 | 0.134 | 0.17 | 0.25 | 0.307 | 0.365 | 0.5 | 0.718 | 0.843 | 1.0 | 1.125 | |
| 12" | 300 | 12.75 | 0.165 | 0.18 | 0.25 | 0.33 | 0.406 | 0.5 | 0.843 | 1.0 | 1.125 | 1.312 | |
API 5L PLS2 ERW TIYO