Gwo Dyamèt Nerjaveèi tiyo
video

Gwo Dyamèt Nerjaveèi tiyo

Dyamèt deyò: gwosè min 1/8 pous, gwosè max 40 pous, DN6 pou DN1000.
Epesè miray: SCH 5, 5S, 10, 10S, 20, 30, 40, 40S, 60, 80, 80S, 100, 120, 140, 160, STD, XS ak XXS, 1.24mm a 25.4mm.
Koupe nan longè: longè o aza ka ofri, longè max ka 20 mèt, ak longè tiyo fiks se 6 mèt.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon
Gwo dyamèt Nerjaveèi tiyo Deskripsyon

Tiyo asye pur ak yon dyamèt deyò ki pi gran pase 200 mm (8 pous) vin gwo-dyamèt tiyo asye pur, ki souvan itilize pou transpòte gaz natirèl, lwil oliv ak sou sa.
Gwoup GNEE, kòm yon manifakti pwofesyonèl gwo dyamèt asye pur, gen 3 gwo dyamèt liy pwodiksyon tiyo asye pur ak 2 ti dyamèt liy pwodiksyon tiyo asye pur. Nou ka bay estanda tiyo asye pur tankou A312, A358, A269, A789, elatriye Nou ka bay pwosesis pwodiksyon tankou tiyo asye pur, poli asye pur tiyo san pwoblèm, Nerjaveèi asye electrofusion soude tiyo, Nerjaveèi asye rezistans soude tiyo, Nerjaveèi. asye wonn tiyo, asye pur tiyo rektangilè, elatriye Nou ka ofri pi ba pri pase lòt founisè, si w enterese, ou ka kontakte nou pou sitasyon pi ba.

Gwo Dyamèt Nerjaveèi Tib Spesifikasyon

Spesifikasyon ASTM A312, ASTM A778, ASTM A358, ASTM A999
Estanda ASTM, ASME ak API
Gwosè EFW - 8" NB TO 110" NB (Gwosè Nominal twou)
Kalite Elektrik-Fizyon-soude, san pwoblèm, Polonè, elatriye.
Longè 01 mèt a 12.5 mèt, yon sèl longè o aza, doub longè o aza ak Customize gwosè.
Dyamèt Eksteryè 6.00 mm OD jiska 914.4 mm OD, gwosè jiska 24" NB
Epesè miray la (3 mm rive 100 mm epesè) SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Fen Plain Fen, Bizote Fen, Treaded
Tèm Peman T/T, L/C, ETC.

Klas tiyo asye pur

Klas Kabòn Silisyòm Manganèz Kwòm Nikèl Molybdène Souf Fosfò
TP304 0,08 1,0 2.00 18.0 – 20.0 8.0 – 11.0 – 0,03 0,045
TP304L 0,035 1,0 2.00 18.0 – 20.0 8.0 – 13.0 – 0,03 0,045
TP316 0,08 1,0 2.00 16.0 – 18.0 10.0 – 14.0 2.00 – 3.00 0,03 0,045
TP316l 0,035 1,0 2.00 16.0 – 18.0 10.0 – 15.0 2.00 – 3.00 0,03 0,045
TP321 0,08 1,0 2.00 17.0 – 19.0 9.0 – 12.0 – 0,03 0,045

Gwo-dyamèt tiyo asye pur pou kanalizasyon endistriyèl

Spesifikasyon pou mezi gwo dyamèt (Specifikasyon ak dimansyon yo se pou ASME B36.19M sèlman)
rebè Dyamèt deyò Epesè miray nominal
SCH 5S SCH 10S SCH 40S
rebè NPS manm manm manm manm
350 14" 355.6 3.96 4.78 9.53
400 16" 406.4 4.19 4.78 9.53
450 18" 457 4.19 4.78 9.53
500 20" 508 4.78 5.54 9.53
550 22" 559 4.78 5.54 -
600 24" 610 5.54 6.35 9.53
750 30" 762 6.35 7.92 -

Pwopriyete mekanik pou gwo tiyo asye pur

Klas Propcrites mekanik
Fòs rupture Yied fòs Elongasyon Dite
KSi (MPa) KSi (MPa) % HRB
ASTM TP304 Mwens pase oswa egal a 75(515) Mwens pase oswa egal a 30(205) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
TP304L Mwens pase oswa egal a 70 (483) Mwens pase oswa egal a 25 (170) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
TP316 Mwens pase oswa egal a 75(515) Mwens pase oswa egal a 30(205) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
TP316l Mwens pase oswa egal a 70 (483) Mwens pase oswa egal a 25 (170) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
ANNWI SUS304 Mwens pase oswa egal a 75 (520) Mwens pase oswa egal a 30(206) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
SUS304L Mwens pase oswa egal a 70 (481) Mwens pase oswa egal a 25(177) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
SUS316 Mwens pase oswa egal a 75 (520) Mwens pase oswa egal a 30(206) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
SUS316L Mwens pase oswa egal a 70 (481) Mwens pase oswa egal a 25(177) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
GB 0Crl8Ni9 Mwens pase oswa egal a 75 (520) Mwens pase oswa egal a 30(210) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
{{0}}Crl9Nil0 Mwens pase oswa egal a 70 (480) Mwens pase oswa egal a 25 (180) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
0Crl7Nil2Mo2 Mwens pase oswa egal a 75 (520) Mwens pase oswa egal a 30(210) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
00Crl7Nil4Mo2 Mwens pase oswa egal a 70 (480) Mwens pase oswa egal a 25 (180) Mwens pase oswa egal a 35 Mwens pase oswa egal a 90
EN10217-7 1.4301 (500-700) Mwens pase oswa egal a (195) >40b Mwens pase oswa egal a 90
1.4307 (470-670) Mwens pase oswa egal a (180) >40b Mwens pase oswa egal a 90
1.4401 (510-710) Mwens pase oswa egal a (205) >40b Mwens pase oswa egal a 90
1.4404 (490-690) Mwens pase oswa egal a (190) >40b Mwens pase oswa egal a 90

Gwo Dyamèt Steel Tubing

large stainless steel pipe

thick wall stainless steel tube

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

GNEE Pwovizyon pou Kalite tiyo asye pur

Nerjaveèi asye tiyo echapman Tib wonn asye pur
Poli Nerjaveèi tiyo Oval Steel tiyo
Nerjaveèi tiyo san pwoblèm Mens miray Nerjaveèi Tib
Nerjaveèi asye soude tiyo Segondè presyon asye pur tib
Nerjaveèi asye kare tiyo ERW SS tiyo

Poukisa chwazi GNEE SS Steel tiyo?

  1. Gwoup GNEE gen 16 ane eksperyans nan pwodiksyon ak ekipman pou gwo dyamèt tiyo asye pur.
  2. Tiyo asye pur ki te pwodwi pa GNEE yo pi pri-efikas pase sa yo ki te pwodwi pa Metline.
  3. Chak ane, nou bay plis pase 50 milyon tòn tiyo asye pur globalman.
  4. Nou ofri yon sèvis yon sèl-stop pou adrese tout bezwen ou yo, ki gen ladan pwodwi, lojistik, ak anbalaj.
  5. Nou bay SGS, ISO, CE, rapò enspeksyon faktori, ak rapò enspeksyon twazyèm pati.
  6. Pèsonalizasyon nan tiyo asye pur oswa lòt tiyo asye sipòte.

stainless steel pipe supplier

 

Baj popilè: gwo dyamèt Nerjaveèi asye tiyo, Lachin gwo dyamèt Nerjaveèi asye tiyo manifaktirè, Swèd