API 5L X52 X56 ERW Tiyo
video

API 5L X52 X56 ERW Tiyo

Kabòn Steel API 5L X52, X56 liy tiyo souvan refere yo kòm asye kabòn plenn paske alyaj prensipal materyèl la se kabòn.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon

API 5L X52 X56 Linepipe Supplier-GNEE

API 5L X52 X56 ERW tiyo yo itilize nan anviwònman estrès segondè. Materyèl la gen yon fòs rupture minimòm de 520 MPa. Tiyo solid CS API 5L X52 X56 ERW yo pwodui pa yon pwosesis soude rezistans.

 

Gwosè Range 1/2 a 36 pous NB
Ranje epesè orè SCH 40, 80, 160, XS, XXS, Tout Orè yo
Aplikasyon Rafinri lwil oliv, jenerasyon pouvwa, pétrochimique, sik, veso presyon, ekipman chodyè, rezon jeni jeneral
Kalite tiyo ERW, soude
Fòm Tib ak Tib Wonn, kare, rektangilè
Longè: Single, Double Random & Length, Custom Size - 12 M longè
Fen: Bizote Fen, Plain Fen, Treaded
Pwoteksyon fen: Bouchon plastik
Fin Koneksyon pou Tiyo Liy Plain, Bizote, Vise, Threaded
Deyò kouch Nwa Penti, Anti-Korozyon lwil oliv, galvanize Fini

 

PSL 1
Klas Konpozisyon chimik Pwopriyete mekanik
C (Max) Mn (Max) P (Max) S (Maks) TENSILE (Min) RENDISMAN (Min)
Psi X 1000 Mpa Psi X 1000 Mpa
A25 CL I 0.21 0.60 0.030 0.030 45 310 25 172
CL II 0.21 0.60 0.030 0.030
A 0.22 0.90 0.030 0.030 48 331 30 207
B 0.26 1.20 0.030 0.030 60 414 35 241
X42 0.26 1.30 0.030 0.030 60 414 42 290
X46 0.26 1.40 0.030 0.030 63 434 46 317
X52 0.26 1.40 0.030 0.030 66 455 52 359
X56 0.26 1.40 0.030 0.030 71 490 56 386
X60 0.26 1.40 0.030 0.030 75 517 60 414
X65 0.26 1.45 0.030 0.030 77 531 65 448
X70 0.26 1.65 0.030 0.030 82 565 70 483

 

PSL 2
Klas Konpozisyon chimik Pwopriyete mekanik
C
(Maks)
Mn
(Maks)
P
(Maks)
S
(Maks)
tansyon Sede ENERGI IMPACT CE
Psi x 1000 Mpa Psi x 1000 Mpa PCM IIW J FT/LB
B 0.22 1.20 0.025 0.015 60 - 110 414 - 758 35 - 65 241 - 448 0.25 0.43 T/L 27/41 T/L 20/30
X42 0.22 1.30 0.025 0.015 60 - 110 414 - 758 42 - 72 290 - 496 0.25 0.43 T/L 27/41 T/L 20/30
X46 0.22 1.40 0.025 0.015 63 - 110 434 - 758 46 - 76 317 - 524 0.25 0.43 T/L 27/41 T/L 20/30
X52 0.22 1.40 0.025 0.015 66 - 110 455 - 758 52 - 77 359 - 531 0.25 0.43 T/L 27/41 T/L 20/30
X56 0.22 1.40 0.025 0.015 71 - 110 490 - 758 56 - 79 386 - 544 0.25 0.43 T/L 27/41 T/L 20/30
X60 0.22 1.40 0.025 0.015 75 - 110 517 - 758 60 - 82 414 - 565 0.25 0.43 T/L 27/41 T/L 20/30
X65 0.22 1.45 0.025 0.015 77 - 110 531 - 758 65 - 82 448 - 565 0.25 0.43 T/L 27/41 T/L 20/30
X70 0.22 1.65 0.025 0.015 82 - 110 565 - 758 70 - 82 483 - 565 0.25 0.43 T/L 27/41 T/L 20/30
X80 0.22 1.90 0.025 0.015 90 - 120 621 - 827 80 - 102 552 - 705 0.25 0.43 T/L 27/41 T/L 20/30

 

API 5L X52 X56 ERW Tiyo Pipe ekspozisyon

hollow steel pipethin wall steel pipe

Baj popilè: api 5l x52 x56 erw tiyo, Lachin api 5l x52 x56 erw tiyo manifaktirè, Swèd

Voye rechèch

whatsapp

skype

Mel

Rechèch