ASTM A135 GrA GrB ERW Steel Tib
Yo itilize tiyo asye ASTM A135 ERW pou transmèt gaz, vapè, dlo oswa lòt likid. Li se tou itilize pou distribisyon dlo oswa aplikasyon pou mete valv nan sistèm pwoteksyon dife ki baze sou dlo, tankou mouye, sèk, pre-aksyon oswa sistèm awozwa.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon
ASTM A135 GrA GrB ERW Tubes Supplier-GNEE
Espesifikasyon sa a kouvri de klas tiyo asye soude ak rezistans, NPS 2 jiska NPS 30 enklizif, ak epesè miray nominal (mwayèn) jiska 0.500 pous. (12.70 mm) ak gwosè nominal soti nan 3/4 a 5 pous. (19 a 127 mm), ak epesè miray nominal (mwayèn) nan 0.083 pous (2.11 mm) a 0.314 pous (3.40 mm), tou depann de gwosè.
| astm A135 / sa135 Tiyo & Tib Size | Pou Tiyo-NPS 1/4″ – 30″ OD, Custom Size Disponib Pou Tib – 6.35mm od to 101.60mm od |
|---|---|
| Tiyo echanjeur chalè & tiyo kondansasyon Klas | ASTM A135 Tiyo & Tiyo, ASME SA135 Tiyo & Tiyo |
| Kalite | San pwoblèm A135 Tiyo & Soude A135 Tiyo, ASTM A135 ERW (Elèktrik Rezistans Soude) Tiyo |
| Longè | Double Random & Obligatwa Longè, Single Random, & Custom Size Disponib |
| Fòm/Fòm | Kare A135 Tiyo, Rektangilè / Rektang SA135 Tiyo, Round SA135 Tiyo & Tib, Mawonnen Tib, "U" Fòm Tiyo & Tib. |
| Tiyo & Tib Fen | Plain Fen, Bizote Fen, Treaded Pwoteje ak bouchon plastik |
| Kouch nan A120 tiyo ak tib | Lwil anti-korozyon, fini galvanize, penti nwa, fini selon kondisyon kliyan yo |
| Dyamèt | NPS ¼ "a 30" dyamèt, Dyamèt Custom Disponib |
| Klas | A135 Klas A, A135 Klas B |
| Orè | 5, 10, 20, 30, 40, 60, 80, 100, 120, 14000, XS, XXS, STD |
Gwosè ki disponib pou tiyo asye limyè miray (tiyo Sch10)
| Gwosè | Epesè (mm) | Tès presyon (MPa) | Ref. Non. |
|---|---|---|---|
| 3/4″ / DN20 2f 26.7mm | 2.11 | 17.2 | P0302 (FM) |
| 1% e2�% b3 / DN25 / 33.4mm | 2.77 | 17.2 | P0303 (FM) |
| 1-1/4″ / DN32 / 42.2mm | 2.77 | 17.2 | P0304 (FM) |
| 1-1/2″ / DN40 / 48.3mm | 2.77 | 16.5 | P0305 (FM) |
| 2% e2% 80� / DN50 % 2f 60.3mm | 2.77 | 13.1 | P0306 (FM) |
| {{0}}}/2″ / DN65 / 73.0mm | 3.05 | 11.7 | P0307 (FM) |
| 3% e2% 80� / DN80 % 2f 88.9mm | 3.05 | 9.6 | P0308 (FM) |
| 4�% 80� / DN100 % 2f 114.3mm | 3.05 | 7.6 | P0309 (FM) |
| 5% e2�� / DN125 / 141.3mm | 3.40 | 6.9 | P0310 (FM) |
| 6% e2% 80� / DN150 % 2f 168.3mm | 3.40 | 5.8 | P0311 (FM) |


Baj popilè: astm a135 gra grb erw asye tib, Lachin astm a135 gra grb erw asye tib manifaktirè, Swèd