Segondè presyon asye pur priz Weld Tee
video

Segondè presyon asye pur priz Weld Tee

Tee yo rele tou tiyo Fitting Tee oswa Tee Fitting, Tee jwenti, elatriye Li se sitou itilize chanje direksyon an nan likid epi yo itilize nan tiyo branch nan tiyo prensipal yo. Ka klase selon dyamèt tiyo. Anjeneral te fè nan asye kabòn, asye jete, asye alyaj, asye pur, kòb kwiv mete, alyaj aliminyòm, plastik, agon, PVC ak lòt materyèl.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon

Gen de souvan itilize tee-wo presyon, youn se soude Tee-wo presyon, ak lòt la se entegral fòje Tee-wo presyon. Soude tees wo-presyon yo te fè nan-wo kalite tiyo asye wo-presyon. Metòd fabrikasyon an se menm jan ak fouye twou nan tiyo yo. Twou yo nan tiyo prensipal la dwe konsistan avèk dyamèt tiyo branch ki konekte yo. Kondisyon bon jan kalite soude yo strik. Prechofaj anjeneral obligatwa anvan soude, epi tretman chalè fèt apre soude. Espesifikasyon li yo ak ranje presyon yo se menm ak sa yo ki nan koud segondè presyon.

Estanda -ANSI/ASME:ASTM A182% 2c ASTM SA182

Dimansyon:ASME 16.11, MSS SP-79, MSS SP-95, 83, 95, 97, BS 3799

Gwosè:1/8" NB POU 4" NB

Klas:2000LBS, 3000LBS, 6000LBS

Kalite:Socket Weld Fitting Tee, Socket Weld Egal Tee, Socket Weld Tee inegal

Spesifikasyon Wotè enpè S S1 D D1 C C1 G Epesè
(Gwo Size)
Epesè
(Ti gwosè)
Pwa
1/2 * 1/4 50 33 22.3 14.5 15 8.5 9.5 9.5 15.5 5.4 9.3 0.4
1/2 * 3/8 50 33 22.3 18 15 11.8 9.5 9.5 15.5 5.4 7.5 0.4
3/4 * 3/8 63 38 27.5 18 20.2 11.8 12.5 9.5 19 5.3 10 0.5
3/4 * 1/2 63 38 27.5 22.3 20.2 15 12.5 9.5 19 5.3 7.9 0.5
1 * 1/2 70 46 34.5 22.3 25.9 15 12.5 9.5 22.5 5.8 11.9 0.7
1 * 3/4 70 46 34.5 27.5 25.9 20 12.5 12.5 22.5 5.8 9.3 0.7
1-1/4 * 1/2 79 57 42.7 22.3 34.3 15 12.5 9.5 27 7.2 17.4 1.2
1-1/4 * 3/4 79 57 42.7 27.5 34.3 20.2 12.5 12.5 27 7.2 14.8 1.1
1-1/4 * 1 79 57 42.7 34.5 34.3 25.9 12.5 12.5 27 7.2 11.3 1.1
1-1/2 * 1/2 89 63 48.8 22.3 40.1 15 12.5 9.5 32 7.1 20.4 1.5
1-1/2 * 3/4 89 63 48.8 27.5 40.1 20.2 12.5 12.5 32 7.1 17.8 1.4
1-1/2 * 1 89 63 48.8 34.5 40.1 25.9 12.5 12.5 32 7.1 14.3 1.3
1-1/2 * 1-1/4 89 63 48.8 42.7 40.1 34.3 12.5 12.5 32 7.1 10.2 1.2
2 * 1/2 108 76 60.8 22.3 51.7 15 16 9.5 38 7.6 26.9 2.4
2 * 3/4 108 76 60.8 27.5 51.7 20.2 16 12.5 38 7.6 24.3 2.3
2 * 1 108 76 60.8 34.5 51.7 25.9 16 12.5 38 7.6 10.8 2.2
2 * 1-1/4 108 76 60.8 42.7 51.7 34.3 16 12.5 38 7.6 16.7 2.1
2 * 1-1/2 108 76 60.8 48.8 51.7 40.1 16 12.5 38 7.6 13.6 2

Tee asye pur