Alloy Steel ASTM A234 Klas WP5
video

Alloy Steel ASTM A234 Klas WP5

A234 se yon materyèl estanda Ameriken ak yon estanda Ameriken pou asye kabòn fòje ak ekipman tiyo asye alyaj pou tanperati mwayen ak segondè. Estanda A234 la gen ladan asye kabòn ak klas asye alyaj tankou WPB, WP5, WP9, WP11, WP12, WP22, ak WP91.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon

ASTM A234 se yon spesifikasyon estanda pibliye pa Sosyete Ameriken pou Tès ak Materyèl (ASTM) ki dekri kondisyon fabrikasyon pou ekipman tiyo asye kabòn ak alyaj. Nan Lachin, estanda nasyonal ki koresponn lan se GB/T12459.

Espesifikasyon:ANSI/ASME B16.9, B16.28, MSS-SP-43.

Estanda:ASTM A234 / ASME SA234

Gwosè:½"NB rive 48"NB nan Sch 10s, 40s, 80s, 160s, XXS.

Orè :Sch.40 rive Sch.XXs

Kalite:San pwoblèm / soude

Konpozisyon chimik ASTM A234 Alloy Steel tiyo Fittings (%)

Klas C Mn P S sizo Kr Mouvman Lòt moun
WP1 0.28 0.30-0.90 0.045 0.045 0.10-0.50 - 0.44-0.65 -
WP12 CL1, WP12 CL2 0.05-0.20 0.30-0.80 0.045 0.045 0.60 0.80-1.25 0.44-0.65 -
WP11 CL1 0.05-0.15 0.30-0.60 0.030 0.030 0.50-1.00 1.00-1.50 0.44-0.65 -
WP11 CL2, WP11 CL3 0.05-0.20 0.30-0.80 0.040 0.040 0.50-1.00 1.00-1.50 0.44-0.65 -
WP22 CL1, WP22 CL3 0.05-0.15 0.30-0.60 0.040 0.040 0.50 1.90-2.60 0.87-1.13 -
WP24 0.05-0.10 0.30-0.70 0.020 0.010 0.15-0.45 2.20-2.60 0.90-1.10 *A
WP5 CL1% 2c WP5 CL3 0.15 0.30-0.60 0.040 0.030 0.50 4.0-6.0 0.44-0.65 -
WP9 CL1% 2c WP9 CL3 0.15 0.30-0.60 0.030 0.030 1.00 8.0-10.0 0.90-1.10 -
FLÈV 0.20 0.40-1.06 0.045 0.050 - - - *B
WP91 0.08-0.12 0.30-0.60 0.020 0.010 0.20-0.50 0.85-1.05 0.85-1.05 *C
WP911 0.09-0.13 0.30-0.60 0.020 0.010 0.10-0.50 0.90-1.10 0.90-1.10 *D
WP92 0.07-0.13 0.30-0.60 0.020 0.010 0.50 0.30-0.60 0.30-0.60 *E

Pwopriyete mekanik ASTM A234 Alloy Steel tiyo Fittings

Klas Fòs rupture, min. ksi[MPa] Sede fòs, min. ksi[MPa] Elongasyon, min. %
Lonjitidinal Transvèse
WP1 55-80[380-550] 30[205] 20 13
WP12 CL1 60[415] 32[220] 22 14
WP12 CL2 70[485] 40[275] 22 14
WP11 CL1 60[415] 30[205] 22 14
WP11 CL2 70[485] 40[275] 22 14
WP11 CL3 75[520] 45[310] 22 14
WP22 CL1 60[415] 30[205] 22 14
WP22 CL3 75[520] 45[310] 22 14
WP24 85[585] 60[415] 20 -
WP5 CL1 60[415] 30[205] 22 14
WP5 CL3 75[520] 45[310] 22 14
WP9 CL1 60[415] 30[205] 22 14
WP9 CL3 75[520] 45[310] 22 14
FLÈV 63-99[435-605] 46[315] 20 -
WP91 90[620] 60[415] 20 13
WP911 90-120[620-840] 64[440] 20 13
WP92 90-120[620-840] 64[440] 20 13

A234 Fitting tiyo

A234 pipe fittingsA234 WP5 pipe fitting

Baj popilè: alyaj asye astm a234 klas wp5, Lachin alyaj asye astm a234 klas wp5 manifaktirè, Swèd

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch