- API 5CT K55 lwil oliv bwat tiyo se sitou itilize kòm yon tiyo ki bese nan pi a pou pwodiksyon likid oswa piki likid. Apre perçage fini, lwil brit ak gaz natirèl yo transpòte soti nan kouch lwil oliv ak gaz nan sifas la.
- API 5CT K55 Aman Tib Konpozisyon Chimik, fraksyon mas (%)
| Klas | Kalite | C | Mn | Mouvman | Kr | Ni max. | Cu max. | P max. | S max. | Si max. | ||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| min. | max. | min. | max. | min. | max. | min. | max. | |||||||
|
K55 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
0.03 |
0.03 |
- |
- API 5CT K55 Aman tib Pwopriyete mekanik
| Estanda | Kalite | Fòs rupture MPa | Sede Fòs MPa | Dite Max. |
|---|---|---|---|---|
| API SPEC 5CT | K55 | Pi gran pase oswa egal a 517 | Pi gran pase oswa egal a 655 | --- |