Seksyon kre galvanize

Pwodwi Deskripsyon

Non: GI Hollow Section

Sifas: galvanize (40-60g/m2 nòmal, kliyan ka mande l)

OD:10*15-100*150mm

WT:0.{6-2.3mm

Longè: fiks oswa o aza, kòm demann kliyan

Fòm: rektangilè

Materyèl: Q195 Q215 Q235

Kondisyon komès: FOB, C&F, CIF, EXW

Regleman Peman: TT depo + BL kopi / LC oswa 100% LC nan je

Espesifikasyon seksyon kre

Gwosè kg/m Longè Mill Std (m)
13x13x1.8mm ** 0.57 6.5
15x15x1.8mm ** 0.68 6.5
20x20x1.6mm 0.87 6.5
25x25x1.6mm 1.12 6.5
25x25x2.{{3}mm 1.36 6.5
25x25x2.5mm 1.64 6.5
25x25x3.{{3}mm 1.89 6.5
30x30x1.6mm 1.38 8.0
30x30x2.0mm 1.68 8.0
30x30x2.5mm 2.03 8.0
30x30x3.0mm 2.36 8.0
35x35x1.6mm 1.63 8.0
35x35x2.0mm 1.99 8.0
35x35x2.5mm 2.42 8.0
40x40x1.6mm 1.88 8.0
40x40x2.0mm 2.31 8.0
40x40x2.5mm 2.82 8.0
40x40x3.0mm 3.30 8.0
40x40x4.0mm 4.09 8.0
50x50x1.6mm 2.38 8.0
50x50x2.0mm 2.93 8.0
50x50x2.5mm 3.60 8.0
50x50x3.0mm 4.25 8.0
50x50x4.0mm 5.35 8.0
50x50x5.0mm 6.56 8.0
65x65x1.6mm 3.31 8.0
65x65x2.{{3}m 3.88 8.0
65x65x2.5mm 4.78 8.0
65x653.0mm 5.66 8.0
65x65x4.{{3}mm 7.23 8.0
75x75x2.5mm 5.56 8.0
75x75x3.0mm 6.60 8.0, 9.0, 12.0
75x75x4.{{3}mm 8.49 8.0, 9.0, 12.0
75x75x5.{{3}mm 10.30 8.0
75x75x6.0mm 12.00 8.0
89x89x2.{{3}mm 5.36 8.0, 12.0
100x100x3.0mm 8.96 8.0, 12.0
100x100x4.0mm 11.60 8.0, 12.0
100x100x5.0mm 14.20 8.0
100x100x6.0mm 16.70 8.0
125x125x4.0mm ** 14.80 8.0, 12.0
125x1255.0mm ** 18.20 8.0, 12.0
125x125x6.0mm ** 21.40 8.0, 12.0
150x150x5.0mm ** 22.10 8.0, 12.0
150x150x6.0mm ** 26.20 8.0, 12.0
2{{3}0x200x5.0mm ** 29.90 8.0, 12.0
2{{3}0x200x6.0mm ** 35.60 8.0, 12.0

Rektangilè Steel Tib

MILD STEEL HOLLOW SECTIONSERW Hollow Sections

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Sèvis nou an

1. strik kontwòl pwosesis pou asire ke alè livrezon trepye
2. Nou pral ede ak anbake dokiman yo
3. Enjenyè ansyen nou yo ka bay konsèy enstalasyon, komisyonin, ak sèvis fòmasyon.
4. Manyèl itilizatè angle, manyèl pati, sètifika pwodwi, ak sètifika ki gen rapò yo bay sou livrezon.
5. 12 mwa garanti apre enstalasyon ak komisyonin, eksepte pou faktè domaj imen.
6. Bay konsiltasyon teknik nenpòt lè epi fè enjenyè sèvis machin nan lòt bò dlo.

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch