Sep 24, 2025 Kite yon mesaj

Konsantrik redukteur, ANSI B16.9, DN150 X DN80, SCH 40, BW bato nan Perou

‌ANSI B16.9 konsantrik redukteur‌ (ke yo rele tou yon redukteur konsantrik oswa konsantrik redukteur Fitting) karakterize pa gen dyamèt tiyo diferan nan tou de bout men ak yon liy pataje. Sa a konsepsyon asire yon tranzisyon lis pou koule likid, minimize ajitasyon ak pèt presyon. Konpare ak redukteur inik, redukteur konsantrik yo pi apwopriye pou sistèm tiyo orizontal kote segondè estabilite koule likid ki nesesè.

 

Lòd spesifikasyon

Pwodwi: konsantrikDiminye.
Materyèl: ASTM A403 WP316L.
Gwosè: 6 × 3 pous.
WT: Sch 40.
Creole: ANSI B16.9.
Kalite: san pwoblèm.
Fen: Butt Weld.

 

Redukteur konsantrikDimansyon

3f198ba1eb7064c04f781588f622c7c

Gwosè nominal Dyamèt deyò nan tranchan Sant pou fini
Dn1 DN2 Nps1 Nps2 OD1 OD2 H
20 10-15 3/4 3/8-1/2 26.7 17.1-21.3 38
25 15-20 1 1/2-3/4 33.4 21.3-26.7 51
32 15-25 1 1/4 1/2-1 42.2 21.3-33.4 51
40 15-32 1 1/2 1/2-1 1/4 48.3 21.3-42.2 64
50 20-40 2 3/4-1 1/2 60.3 26.7-48.3 76
65 25-50 2 1/2 1-2 73.0 33.4-60.3 89
80 32-65 3 1 1/4-2 1/2 88.9 42.2-73.0 89
90 32-80 3 1/2 1 1/4-3 101.6 42.2-88.9 102
100 40-90 4 1 1/2-3 1/2 114.3 48.3-101.6 102
125 50-100 5 2-4 141.3 60.3-114.3 127
150 65-125 6 2 1/2-5 168.3 73.0-141.3 140
200 90-150 8 3 1/2-6 219.1 101.6-168.3 152
250 100-200 10 4-8 273.0 114.3-219.1 178
300 125-250 12 5-10 323.8 141.3-273.0 203
350 150-300 14 6-12 355.6 168.3-323.8 330
400 150-350 16 6-14 406.4 168.3-355.6 356
450 200-400 18 8-16 457.0 219.1-406.4 381
500 250-450 20 10-18 508.0 273.0-457.0 508
550 300-500 22 12-20 559.0 323.8-508.0 508
600 300-550 24 12-22 610.0 323.8-559.0 508
650 350-600 26 14-24 660 355.6-610.0 610
700 350-650 28 14-26 711 355.6-660.0 610
750 350-700 30 14-28 762 355.6-711.0 610
800 500-750 32 20-30 813 508.0-762.0 610
850 550-800 34 22-32 864 559.0-813.0 610
900 550-850 36 22-34 914 559.0-864.0 610
950 600-900 38 24-36 965 610.0-914.0 610
1000 700-950 40 28-38 1016 711.0-965.0 610
1050 700-1000 42 28-40 1067 711.0-1016.0 610
1100 800-1050 44 32-42 1118 813.0-1067.0 610
1150 850-1100 46 34-44 1168 864.0-1118.0 711
1200 900-1150 48 36-46 1219 914.0-1168.0 711
1300 1000-1200 52 40-48 1321 1016.0-1219.0 711
1400 1100-1300 56 40-52 1422 1016.0-1321.0 711
1500 1100-1400 60 44-56 1524 1118.0-1422.0 711

concentric-reducer-ansi-b16-9-dn150-x-dn80-sch-40-bw

Kontakte nou pouANSI B16.9 konsantrik redukteur:pipe@gneetube.com

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch