Apr 07, 2024 Kite yon mesaj

ASTM A269 TP 316L Nerjaveèi asye tib san pwoblèm

Pwodwi Deskripsyon

A269 tiyo asye se yon tiyo nominal miray-epesè asye pur itilize nan anviwònman jeneral korozyon ki reziste, ba-tanperati oswa wo-tanperati.

Spesifikasyon ASTM A269 TP316L / ASME SA269 TP316L Tib
Fòm Idwolik, rektangilè, wonn, tib perfectionné, kare, dwat, fòm U, mawonnen, bobin gato chodyè
Sifas fini 400G, BA, 2B, No.8, No.1, No.4, No.3, 500G, 8K, 2D, 1D, 180G, 320G, HL, 400G Saten / Hairline, glas poli, 600G oswa 800G glas fini tib oswa Custom Fini dapre spesifikasyon kliyan an
Kalite Faktori CDS / fabrike / san pwoblèm / CDW / ERW / DOM / CEW / soude / 100% X-Ray soude
Ranje epesè SCH XXS, SCH 10, SCH 5, SCH 40, SCH XXH% 2c SCH XS, SCH 80S, SCH 160, SCH 80
Estanda ASTM, GB, DIN, JIS, AISI, EN, SUS
Teknik Fwad trase, frèt woule, extrusion, cho woule Tib
Kondisyon livrezon Poli, trase frèt, rkwit ak marinated (AP), MF, rkwit klere (BA)
Fen Bizote Fen, Treaded, Plain Fen
Sèvis pwosesis Koupe, Decoiling, koube, soude, pwensonaj, bòdi

Konpozisyon chimik ASTM A269 TP 316L Tib san pwoblèm

KLAS  

C

mn

SIZO

P

S

CR

MO

NI

N

316L

min

-

-

-

-

-

16.0

2.00

10.0

-

Maks

0.03

2.0

0.75

0.045

0.03

18.0

3.00

14.0

0.10

Pwopriyete mekanik ASTM A269 TP 316L ASTM A269 TP316L Tib tiyo echapman asye pur

KLAS TÈS
(MPA) MIN
YDELD STR
0.2% PRÈV
(MPA) MIN
LONG
(% NAN 50MM) MIN
DITE
ROCKWELL B B B) MAX BRINELL (HB) MAX

316L

485

170

40

95

217

ASME SA 269 TP316L Tib san pwoblèm

A269 Austenitic Steel PipeStainless Steel Tube

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 