Deskripsyon
Non pwodwi:Tiyo fant, anvlòp fant, tiyo asye fant
Aplikasyon:Itilize kòm miray estriktirèl Retainers ak tiyo ekran pou lwil oliv, gaz ak dlo Wells
OD:50mm - 500mm
WT:mwens pase 20mm
LONGÈ:mwens pase 15m
Espesifikasyon plas & twou:Kòm kliyan mande
Estanda ak Klas:API 5CT J55/K55/N80/C75/L80/C90/T95/Q125
Kalite pwosesis:San pwoblèm (SMLS), Rezistans elektrik soude (ERW)
Fen:Plain, Bizote, Koupe kare, ak koneksyon LTCISTC/BTC
Sifas:Anti-Korozyon ak Penti Dlo
Anbalaj:Bouchon pwoteksyon nan tou de bout, papye ki enpèmeyab vlope
Fant ak detache sou kò a tiyo yo dwe fè tiyo. Kalite plas yo detache, rektangilè fant, trapèz fant, pon fant, ekran anvlope fil, koupe mekanik, tiyo konpoze. Tiyo fant la ap itilize nan eksplorasyon lwil oliv pou anpeche sab, diminye lwil oliv byen repare, ogmante fòs lwil oliv, entegralite ak estabilite nan kenbe nan sab.
FantAnvlòpEspesifikasyon tiyo
O.D.:Aman: 4 1/2"-20"(114.3mm-508mm); Tib: 1.05 "-41/2" (26.7mm-114.3m)
Longè: R1:4.88-7.62M,R2:7.621-10.36M,R3:10.36-14.63M
W.T.:0.205""-0.875" (5.21mm- 22.22mm)
Estanda pwodwi:API 5CT, BS EN ISO11960, NFM87-207, JIS G3439, ISO 4270, GOST632-80
Materyèl:H40, J55, K55, N80-1, N80Q, R95, L80-1, L80-9Cr, L80-13Cr, C90, T95, C110, P110, Q1252.
Anvlòp:STC, LTC, BTC elatriye.
Tib:NU, EU, XL, PH-4, PH-6, LTC, STC, BTC elatriye.
Avantaj nan Union Steel Slotted tiyo
1. Tiyo detache nou an sèvi ak J55 / K55 / N80 aman ak tib nan estanda API, ak segondè fòs jeneral, pa tèlman fasil deformation.
2. Kwen an nan plas la se vètikal, lis, san burrs, ak plas la se inifòmite.
3. Tiyo a detache se apwopriye pou Sandy byen, ki dyamèt sab la pi gran pase 0.3mm.
4. Fant la ka longitudinal ak transverse, seksyon an nan plas la ka paralèl ak trapezoidal kalite, ak yon zòn gran louvri.
5. Tiyo ekran fant gen yon gwo dyamèt enteryè.
Spesifikasyon
|
API Casing tiyo |
ID |
Longè |
Longè plas |
Plas No. |
Lajè plas |
Fant |
Filtre Valab |
Max. |
||
|
Spec mm |
Epesè |
Pou chak pwa |
||||||||
|
60.32 |
5 |
6.84 |
50.3 |
3 |
80 |
200 |
0.3 |
±50 |
48 |
512.54 |
|
73.02 |
5.5 |
9.15 |
62 |
240 |
57.6 |
688.55 |
||||
|
88.9 |
6.5 |
13.22 |
75.9 |
280 |
67.2 |
995.1 |
||||
|
101.6 |
6.5 |
15.22 |
88.6 |
300 |
72 |
1151.2 |
||||
|
114.3 |
7 |
18.47 |
100.3 |
10 |
320 |
76.8 |
1400.4 |
|||
|
127 |
7.52 |
22.13 |
112 |
340 |
81.6 |
1673.8 |
||||
|
139.7 |
7.72 |
25.11 |
124.3 |
360 |
86.4 |
1900.2 |
||||
|
9.17 |
29.48 |
121.4 |
360 |
86.4 |
2232.4 |
|||||
|
168.3 |
8.94 |
35.09 |
150.4 |
400 |
96 |
2672.95 |
||||
|
177.8 |
8.05 |
33.68 |
161.7 |
440 |
105.6 |
2559.2 |
||||
|
9.19 |
38.19 |
159.4 |
440 |
105.6 |
2940.7 |
|||||
|
Dimansyon tiyo ekran (pous) |
OD (mm) |
Epesè miray (mm) |
ID (mm) |
Nimewo asanblaj chak sèk |
Lajè plas (mm) |
Longè plas (mm) |
Longè (mm) |
|
2-3/8″ |
60.3 |
4.83 |
50.64 |
12~18 |
0.2~0.8 |
45~100 |
1000~12000 |
|
2-7/8″ |
73 |
5.51 |
61.98 |
20~24 |
45~100 |
||
|
3-1/2″ |
88.9 |
6.45 |
76 |
24~28 |
45~100 |
||
|
4″ |
101.6 |
6.65 |
88.29 |
24~30 |
45~100 |
||
|
4-1/2″ |
114.3 |
5.69 |
102.92 |
24~30 |
45~100 |
||
|
6.35 |
101.6 |
45~100 |
|||||
|
7.37 |
99.57 |
45~100 |
|||||
|
8.56 |
97.18 |
45~100 |
|||||
|
5″ |
127 |
5.59 |
115.82 |
28~36 |
0.25~0.8 |
45~100 |
|
|
6.43 |
114.15 |
45~100 |
|||||
|
7.52 |
111.96 |
45~100 |
|||||
|
9.19 |
108.61 |
45~100 |
|||||
|
5-1/2″ |
139.7 |
6.2 |
127.3 |
30~38 |
45~100 |
||
|
6.99 |
125.73 |
45~100 |
|||||
|
7.72 |
124.26 |
45~100 |
|||||
|
9.17 |
121.36 |
45~100 |
|||||
|
10.54 |
118.62 |
45~100 |
|||||
|
7″ |
177.8 |
6.91 |
163.98 |
36~50 |
45~100 |
||
|
8.05 |
161.7 |
45~100 |
|||||
|
9.19 |
159.41 |
45~100 |
|||||
|
10.36 |
157.07 |
45~100 |
Estanda
Konpozisyon chimik nan tiyo Steel Slotted
|
Estanda |
Klas |
Konpozisyon chimik (%) |
|||||||||
|
API SPEC 5CT |
J55 |
C |
Si |
Mn |
P |
S |
Kr |
Ni |
Cu |
Mo |
V |
|
K55 |
0.34-0.39 |
0.20-0.35 |
1.25-1.50 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.015 |
Mwens pase oswa egal a 0.15 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
/ |
/ |
|
|
N80 |
0.34-0.38 |
0.20-0.35 |
1.45-1.70 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.015 |
Mwens pase oswa egal a 0.15 |
/ |
/ |
/ |
0.11-0.16 |
|
|
L80 |
0.15-0.22 |
Mwens pase oswa egal a 1.00 |
0.25-1.00 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.010 |
12.0-14.0 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
/ |
/ |
|
|
P110 |
0.26-0.395 |
0.17-0.37 |
0.40-0.70 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.010 |
0.80-1.10 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
0.15-0.25 |
Mwens pase oswa egal a 0.08 |
|
Pwopriyete mekanik nan tiyo ekran fant
|
Klas |
Kalite |
elongasyon total anba chaj (%) |
Fòs sede (min) |
Fòs sede (max) |
Fòs rupture min Mpa |
Dite Max (HRC) |
Dite Max (HBW) |
|
J55 |
- |
0.5 |
379 |
552 |
517 |
- |
- |
|
K55 |
- |
0.5 |
379 |
552 |
655 |
- |
- |
|
N80 |
1 |
0.5 |
552 |
758 |
689 |
- |
- |
|
N80 |
Q |
0.5 |
552 |
758 |
689 |
- |
- |
|
L80 |
1 |
0.5 |
552 |
655 |
655 |
23 |
241 |
|
L80 |
9Kr |
0.5 |
552 |
655 |
655 |
23 |
241 |
|
L80 |
13Kr |
0.5 |
552 |
655 |
655 |
23 |
241 |
|
C90 |
- |
0.5 |
621 |
724 |
689 |
25.4 |
255 |
|
C95 |
- |
0.5 |
655 |
758 |
724 |
- |
- |
|
T95 |
- |
0.5 |
655 |
758 |
724 |
25.4 |
255 |
|
P110 |
- |
0.6 |
758 |
965 |
862 |
- |
- |
|
Q125 |
Tout |
0.65 |
862 |
1034 |
931 |
- |
- |
Pwosesis


Anbalaj