I. Materyèl Prensipal pou Tib Bobin
Entènasyonalman, bobine tib (CT) pou pwodiksyon lwil prensipalman itilize segondè - fòs ki ba - asye alyaj ak alyaj espesyalite satisfè rezistans korozyon, segondè - tolerans presyon, ak kondisyon rezistans fatig nan anviwònman divès kalite. Materyèl kle ak karakteristik yo:
Asye kabòn
Klas: QT-800, QT-900 (PALECTED & apeze)
Pwopriyete: pri ki ba, fòs modere (80 - 100 ksi sede fòs). Apwopriye pou ba - presyon/ba-tanperati operasyon (<120°C) like routine workovers, sand washing, and acidizing.
Limit: pòv rezistans korozyon; Inoporten pou H₂s/CO₂ pwi asid.
Segondè - fòs ki ba - asye alyaj (HSLA)
Klas: CT-100, CT-110 (100-110 KSI sede fòs)
Properties: Enhanced strength/toughness via micro-alloying (Cr, Mo, Ni). Ideal for deep wells (>4,000 m) ak segondè - operasyon presyon (egzanp, fraktur, CT perçage).
Aplikasyon: Shale gaz fraktur, Deepwater konplete.
Korozyon - alyaj rezistan (CRA)
(1) 13cr martensitic asye pur
Pwopriyete: co₂ - rezistan; Aplikab pou segondè - CO₂ Wells (<150°C).
Limitasyon: H₂s - sansib; tendans SULFIDE estrès fann (SSC).
(2) 22cr/25cr duplex asye pur
Pwopriyete: Reziste H₂s+CO₂ korozyon; Itilize nan jaden asid (egzanp, Mwayen Oryan, lanmè nò).
Klas: UNS S31803 (22CR), UNS S32750 (25CR).
(3) nikèl - ki baze sou alyaj (Inconel 625/825)
Properties: Extreme corrosion resistance (H₂S, Cl⁻, high-temperature); for ultra-deep wells (>6,000 m) oswa pwi jewotèmal.
Dezavantaj: gwo pri (10 × prim sou asye estanda).
II. Gid seleksyon materyèl
|
Kalite materyèl |
Aplikasyon Rekòmande |
Senaryo ki pa apwopriye |
|---|---|---|
|
Steel Kabòn (QT-800) |
Fon byen netwayaj, leve nitwojèn |
Pwi asid (H₂s/CO₂), HPHT Wells |
|
HSLA (CT-110) |
Gwo twou san fon - Oke fraktur, CT perçage |
Anviwònman trè korozivite |
|
13cr pur |
Inondasyon co₂, mitan - ba piki tanperati vapè |
High H₂S environments (>50 ppm) |
|
22cr/25cr duplex |
Jaden asid (egzanp, Mwayen Oryan) |
Pri - Pwojè sansib |
|
Inconel 625 |
Ultra-deep wells (>150 degre), gaz tounen |
Operasyon woutin (pri ki ba - efikasite) |
Iii. Founisè Global & Tandans
Manifaktirè
Tenaris (Ajantin): HSLA Steels & 13cr CT.
Sandvik (Syèd): Precision 22cr/25cr Duplex asye tib.
Siperyè enèji (US): fatig - Optimize CT-100/110 Seri.
Tandans Teknoloji
Konpoze ki lejè: kabòn - fib - ranfòse CT (egzanp, CFRTP Schlumberger a), 50% rediksyon pwa ak rezistans kowozyon siperyè.
Smart Tubing: Embedded Fiber - detèktè optik pou reyèl - Tan tanperati/siveyans souch.
Iv. Rekòmandasyon seleksyon
Operasyon woutin → CT - 90/100 asye kabòn (pi bon pri-efikasite).
Anviwònman asid (H₂s) → 22cr Duplex oswa Inconel 625.
Ultra - Deep/High - Temp Wells → Nikèl alyaj oswa konpoze.