Deskripsyon
Itilizasyon:Itilize pou transpò likid presyon ba, tankou dlo, gaz, ak lwil oliv. Perçage lwil oliv ak manifakti machin, elatriye.
ERW:Rezistans elektrik soude tiyo
HFI:Segondè Frekans Endiksyon Weld Tiyo
EFW:Fizyon elektrik soude tiyo
Dyamèt deyò:21.3mm - 660.4mm(1/2″–26″)
Epesè mi:1.5 - 22.2mm
Longè:0.3 – 18 M
Detay yo
Estanda:API 5L, API 5CT, ASTM 53, EN10217, DIN 2458. IS 3589, JIS G3452, BS1387
Steel Klas
API 5L: GR B, X42,X46, X56, X60,X65,X70
ASTM A53: GR A, GR B, GR C
EN: S275, S275JR, S355JRH, S355J2H
GB: Q195, Q215, Q235, Q345, L175, L210, L245, L320, L360- L555
Sifas:Fusion Bond epoksidik kouch, epoksidik goudwon chabon, 3PE, disparisyon kouch, kouch bitumen, kouch lwil nwa (selon kondisyon kliyan an)
Tès:Analiz konpozan chimik, Pwopriyete Mekanik (Fòs Tensile Ultim, Fòs Sede, elongasyon), Mekanik (Tès Flattening, Tès koube, Tès Enpak), Dimansyon&Tcheke vizyèl, Tès idrostatik.
Sètifika Tès Mill:EN10204 3.1
Pwojè ki gen rapò
Tanpri kontakte nou pou plis enfòmasyon
| ane 2023 | Malezi | 394 tòn | Pwojè transmisyon gaz nan Shell, API 5L PSL1 X52, ERW tiyo asye, (SK 115) |
| ane 2022 | Katar | 457.7 tòn | Estasyon pouvwa gouvènman Katar, API 5L PSL1 X65, ERW, tiyo asye, (SK167) |
| ane 2021 | Chili | 2400 tòn | Transmisyon dlo, API 5L L245/ASTM A53 GR.B 406.4/711 ak deyò 3LPE ak andedan FBE, ERW asye tiyo, (YS027) |
| ane 2020 | Lejip | 1042 tòn | Konstriksyon estasyon tren, EN10210 S355JH, tiyo asye ERW, (JH260) |
| ane 2020 | Ostrali | 1400 tòn | Transporasyon likid, API 5L PSL2 X42 ERW tiyo ak Victaulic Groove + Bride + Viraj (AF038) |
| ane 2019 | Nouvèl Zeland | 4700 tòn | Konstriksyon prizon,API 5L PSL1 Gr.B, ERW tiyo asye, (AL226) |
| ane 2018 | Ostrali | 435 tòn | Pwojè Tinèl Ostralyen,API 5L PSL1 X42, ERW tiyo asye, (CLT225) |
| ane 2017 | USA | 700 tòn | Tiyo lwil oliv, API 5L PSL1 X42, ERW tiyo asye |