info-1-1info-1-1

Estanda: API 5L PLS1/ PSL 2

Aplikasyon: Pou gaz, dlo, transpò nan petwòl ak endistri gaz natirèl

 

Tolerans sou dimansyon

Estanda

Soti DyamètEpesè miray la
API 5LToleransTolerans
D<60.3+0.41mm, -0.80mm+15.0%, -12.5%
D≥60.3+0.75%D, -0.75%D+15.0%, -12.5%

 

Estanda

EstandaKlasKonpozan chimik (%)Pwopriyete mekanik
CSiMnPSFòs rupture (Mpa)Sede fòs (Mpa)
API 5L PSL1A0.22-0.900.0300.030≥331≥207
B0.28-1.200.0300.030≥414≥241
X420.28-1.300.0300.030≥414≥290
X460.28-1.400.0300.030≥434≥317
X520.28-1.400.0300.030≥455≥359
X560.28-1.400.0300.030≥490≥386
X600.28-1.400.0300.030≥517≥448
X650.28-1.400.0300.030≥531≥448
X700.28-1.400.0300.030≥565≥483
API 5L PSL2B0.24-1.200.0250.015≥414≥241
X420.24-1.300.0250.015≥414≥290
X460.24-1.400.0250.015≥434≥317
X520.24-1.400.0250.015≥455≥359
X560.24-1.400.0250.015≥490≥386
X600.24-1.400.0250.015≥517≥414
X650.24-1.400.0250.015≥531≥448
X700.24-1.400.0250.015≥565≥483
X800.24-1.400.0250.015≥621≥552