KS D3562 Steel tiyo

KS D3562 Steel tiyo pou sèvis presyon

Tiyo asye KS D3562 yo fèt ak fabrike an akò strik ak estanda Koreyen KS D3562 "Kabòn Steel Tiyo pou Sèvis Presyon". Tiyo sa yo enjenyè pou satisfè egzijans pou transpòte likid anba presyon, sa ki fè yo tounen yon patikil nan divès endistri yo.

KS D3562, entwodwi pwopriyete yo, konpozan, ak aplikasyon nan Kore di estanda soude KS D 3562 SPPS38 tiyo asye ak tib.

 

OD: 10.5-660.4mm
WT: SCH10-80
Klas: SPPS370, SPPS410

Aplikasyon: itilize pou sèvis presyon nan yon tanperati maksimòm apeprè 350

 

Klas ki disponib ak kondisyon livrezon
Klas Estanda: E215, E235, E355

Ka -Fè di: C10E, C15E

Trempe ak apeze Steels: C22E, C35E, C45E

Asye alyaj: 25CrMo4, 30CrMo4, 34CrMo4, 42CrMo4

Kondisyon livrezon:

+C (Travay frèt)

+C +SR (Fwad travay ak estrès-soulaje)

+N (normalize)

+QT (Tèmpe ak Tanperaman) - pou klas alyaj

 

KS D3562 Steel Pipe konpozisyon chimik:

Steel Klas Konpozisyon chimik (%)
C Si Mn P S
SPPS 370 0.25 max. 0.35 max. 0.30 a 0.90 0.040 max. 0.040 max.
SPPS 410 0.30 max. 0.35 max. 0.30 pou 1.00 0.040 max. 0.040 max.

 

KS D3562 Steel tiyo pwopriyete mekanik:

Steel Klas Fòs rupture Sede fòs Elongasyon %
MPa MPa Pa gen . 11 oswa Non. 12 pyès tès Pa gen . 5 pyès tès Pa gen . 4 pyès tès
Longitudinal Transverse Longitudinal Transverse
STPL 370 38{373}min. 22{216} min. 30 min. 25 min. 23 min. 28 min.
STPL 410 42{451} 25{245} min. 25 min. 20 min. 19 min. 24 min.

 

KS D3562 Steel tiyo dimansyon:

DN NPS OD Epesè nominal
Sch 10 Sch 20 Sch 30 Sch 40 Sch 60 Sch 80
A B T Mas inite T Mas inite T Mas inite T Mas inite T Mas inite T Mas inite
mm mm kg/m mm kg/m mm kg/m mm kg/m mm kg/m mm kg/m
6 1/8 10.5 - - - - - - 1.7 0.369 2.2 0.45 2.4 0.479
8 1/4 13.8 - - - - - - 2.2 0.629 2.4 0.675 3 0.799
10 3/8 17.3 - - - - - - 2.3 0.851 2.8 1 3.2 1.11
15 1/2 21.7 - - - - - - 2.8 1.31 3.2 1.46 3.7 1.64
20 3/4 27.2 - - - - - - 2.9 1.74 3.4 2 3.9 2.24
25 1 34 - - - - - - 3.4 2.57 3.9 2.89 4.5 3.27
32 1 1/4 42.7 - - - - - - 3.6 3.47 4.5 4.24 4.9 4.57
40 1 1/2 48.6 - - - - - - 3.7 4.1 4.5 4.89 5.1 5.47
50 2 60.5 - - 3.2 4.52 - - 3.9 5.44 4.9 6.72 5.5 7.46
65 2 1/2 76.3 - - 4.5 7.97 - - 5.2 9.12 6 10.4 7 12
80 3 89.1 - - 4.5 9.39 - - 5.5 11.3 6.6 13.4 7.6 15.3
90 3 1/2 101.6 - - 4.5 10.8 - - 5.7 13.5 7 16.3 8.1 18.7
100 4 114.3 - - 4.9 13.2 - - 6 16 7.1 18.8 8.6 22.4
125 5 139.8 - - 5.1 16.9 - - 6.6 21.7 8.1 26.3 9.5 30.5
150 6 165.2 - - 5.5 21.7 - - 7.1 27.7 9.3 35.8 11 41.8
200 8 216.3 - - 6.4 33.1 7 36.1 8.2 42.1 10.3 52.3 12.7 63.8
250 10 267.4 - - 6.4 41.2 7.8 49.9 9.3 59.2 12.7 79.8 15.1 93.9
300 12 318.5 - - 6.4 49.3 8.4 64.2 10.3 78.3 14.3 107 17.4 129
350 14 355.6 6.4 55.1 7.9 67.7 9.5 81.1 11.1 94.3 15.1 127 19 158
400 16 406.4 6.4 63.1 7.9 77.6 9.5 93 12.7 123 16.7 160 21.4 203
450 18 457.2 6.4 71.1 7.9 87.5 11.1 122 14.3 156 19 205 23.8 254
500 20 508 6.4 79.2 9.5 117 12.7 155 15.1 184 20.6 248 26.2 311
550 22 558.8 6.4 87.2 9.5 129 12.7 171 15.9 213 - - - -
600 24 609.6 6.4 95.2 9.5 141 14.3 228 - - - - - -
650 26 660.4 7.9 103 12.7 203 - - - - - - - -

 

FAQ

1. Ki tanperati opere maksimòm?

Li apwopriye pou aplikasyon pou presyon -pote mwens pase oswa egal a 350 degre. Depase tanperati sa a ka degrade pwopriyete mekanik ak afekte sekirite sistèm lan.

 

2. Èske li ka transpòte likid korozivite?

Materyèl debaz la gen rezistans korozyon debaz. Transpò likid ki trè korozivite mande pou tretman adisyonèl anti-korozyon (tankou kouch epoksidik oswa galvanizasyon).

 

3. Kouman pou mwen chwazi epesè miray ki apwopriye a?

Chwazi selon kondisyon fonksyònman yo: Pou aplikasyon pou gwo-presyon/wo-korozyon, chwazi mi ki pi epè (tankou Sch80); pou aplikasyon pou ba-presyon/ba-korozyon, chwazi miray ki pi mens (tankou Sch10). Tanpri konsilte ekip teknik nou an pou kalkil jeni.

 

4. Èske gen nenpòt gwosè ki pa-estanda?

Nou sipòte gwosè koutim. Tanpri bay KS D3562 Steel Pipe ou dyamèt ekstèn, epesè miray la, ak kondisyon longè. Ekip lavant nou an pral evalye posibilite epi bay yon quote.

 

5. Ki tan livrezon tipik la?

Pou espesifikasyon estanda, tan an se 15-30 jou. Pou lòd ki pa estanda / gwo, ajisteman yo fèt ki baze sou orè pwodiksyon an. Tan an livrezon espesifik ka konfime lè w ap mete yon lòd.

info-712-712

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch