1. Materyèl Konpozisyon & Kle Pwopriyete
Q:Ki sa ki defini pwopriyete chimik/mekanik nan asye E275?
A:
Chimik (wt%):
C:Mwens pase oswa egal a 0.20 |Mn: 0.50–1.40 | P:Mwens pase oswa egal a 0.025 |S:Mwens pase oswa egal a 0.020.
Mekanik:
Fòs Sede (σᵧ):Pi gran pase oswa egal a 275 MPa |Tensile (σₜ):410-560 MPa.
Elongasyon (A₅):Pi gran pase oswa egal a 22% |Dite:Mwens pase oswa egal a 160 HB.
Nòt:E275 se yon asye ki pa -alyajpi bon fòspase E235 men soudabilite menm jan an (Ceq mwens pase oswa egal a 0.40).
2. Faktori & Estanda
Q:Ki jan tib sa yo pwodui ak sètifye?
A:
Pwosesis:San pwoblèm (cho/frèt-fini) oswa soude (ERW/SAW).
Tretman chalè:Nòmalize (EN 10297-1 §6.2) oswa soulaje estrès.
Estanda kle:EN 10297-1 (Aplikasyon mekanik/jeni).
3. Dimansyon tolerans
Q:Ki devyasyon dimansyon yo pèmèt?
A:
| Paramèt | Tolerans |
|---|---|
| OD (D) | ± 1.0% (min ± 0.5 mm) |
| Epesè miray la | ± 10% (min ± 0.3 mm) |
| Dwat | Mwens pase oswa egal a 1.5 mm/m (frèt-desine: Mwens pase oswa egal a 1.0) |
4. Aplikasyon & Limitasyon
Q:Ki kote yo itilize E275 anjeneral?
A:
Estriktirèl:Boom teknik, woulèt transporteur (san pwoblèm).
Sistèm likid:Ba-idwolik presyon (soude, si koule-teste).
Evite: High-temperature (>400 degre) oswa anviwònman asid.
5. Validasyon Kalite
Q:Ki jan kalite asire?
A:
Tès:Tensile (EN ISO 6892-1), dite (EN ISO 6506-1).
Sètifikasyon:EN 10204 3.1/3.2|PED 2014/68/EU pou itilize presyon.
NDT:Opsyonèl UT (EN 10246-1) pou aplikasyon kritik.