Ki diferans ki genyen ant ASTM A53 ak A795?

 ASTM A795 kont ASTM A53 (Gr. B)

Atik / Pwopriyete ASTM A795 (SA795) ASTM A53 Klas B Diferans kle yo
Konpozisyon chimik  
Kabòn (C) 0.20% - 0.25% Mwens pase oswa egal a 0.30% A795 gen kontwòl pi sevè sou kontni kabòn ak yon seri pi etwat.
Manganèz (Mn) 1.15% - 1.50% 0.29% - 1.06% A795 gen kontni Manganèz siyifikativman pi wo, bay efè ranfòsman aparan.
Molybdène (Mo) 0.45% - 0.60% Mwens pase oswa egal a 0.15% (anjeneral trè ba) A795 gen siyifikatif molybdène, pandan y ap A53 pa gen prèske okenn.
Nikèl (Ni) 0.40% - 0.60% Mwens pase oswa egal a 0.40% (anjeneral trè ba) A795 gen nikèl enpòtan, pandan y ap A53 pa gen prèske okenn.
Kwòm (Cr) 0.80% - 1.10% Mwens pase oswa egal a 0.40% (anjeneral trè ba) A795 gen chromium enpòtan, pandan y ap A53 pa gen prèske okenn.
Fosfò (P) Mwens pase oswa egal a 0.025% Mwens pase oswa egal a 0.035% A795 gen kontwòl pi sevè sou fosfò a enpurte.
Souf (S) Mwens pase oswa egal a 0.010% Mwens pase oswa egal a 0.035% A795 gen kontwòl pi sevè sou souf enpurte a.
Pwopriyete mekanik  
Fòs rupture 620 MPa - 795 MPa Pi gran pase oswa egal a 415 MPa Egzijans fòs pou A795 pi wo pase sa pou A53.
Sede fòs Pi gran pase oswa egal a 485 MPa Pi gran pase oswa egal a 240 MPa Fòs sede nan A795 se plis pase de fwa ke nan A53.
Elongasyon Anjeneral pi gwo pase oswa egal a 16% -20% (depann sou espesifikasyon) Egzije pi gwo pase oswa egal a 23% (espécimen lonjitidinal) A53 gen yon kondisyon relativman pi wo pou plastisit.

 