Oct 29, 2025 Kite yon mesaj

Fwad-Materyo Tib Precision Desine

1. Klas Materyèl Prensipal

Q:Ki kalite asye yo itilize pou-tib presizyon frèt?
A:

Asye kabòn:

ASTM A519 1020/1026 (bi jeneral, σᵧ Pi gran pase oswa egal a 350 MPa).

DIN 2391 St35/St52 (Almay), JIS G3445 STKM 13A (Japon).

Asye alyaj:

4130/4140 (Cr-Mo, pou aplikasyon pou gwo -fòs, dite 200-300 HB).

Nerjaveèi asye:

304/316 (ASTM A312) pou rezistans korozyon.

Nòt:E355 (EN 10305-1) se yon klas Ewopeyen komen pou sistèm idwolik yo.


2. Kontwòl Konpozisyon Chimik

Q:Ki limit konpozisyon kritik?
A:

Eleman Limit (poids%) Objektif
C 0.18–0.28 Balanse fòs / duktilite
S/P Mwens pase oswa egal a 0.025 Anpeche frajil
Mn 0.75–1.50 Amelyore hardenability
Kle:Enpurte ki ba (O/N mwens pase oswa egal a 30 ppm) asire estabilite frèt -desen.    

3. Faktori & Tretman Chalè

Q:Kouman yo trete tib sa yo?
A:

Desen frèt:Diminye OD / epesè miray pa 20-40% pou tolerans pi sere.

Recuit:700-850 degre pou soulaje estrès (ISO 10763).

Fini sifas:Manje (Ra mwens pase oswa egal a 0.8 µm) oswa polisaj (Ra mwens pase oswa egal a 0.4 µm).
Rezilta:Fòs rupture 500-800 MPa ak mikrostruktur inifòm.


4. Dimansyon tolerans

Q:Ki nivo presizyon yo reyalize?
A:

Paramèt Tolerans Estanda
OD ± 0.05 mm (ISO 3304) ± 0.1 mm (ASTM A519)
Epesè miray la Mwens pase oswa egal a 3% varyasyon Mwens pase oswa egal a 5% (kalite soude)
Dwat Mwens pase oswa egal a 0.1 mm/m (lazè -verifye) Mwens pase oswa egal a 0.3 mm/m (debaz)

5. Validasyon Kalite & Sètifikasyon

Q:Ki jan kalite asire?
A:

NDT:Eddy aktyèl (ISO 10893-1), tès ultrasons.

Tès mekanik:Tensile (ASTM E8), dite (HRB 70-90).

Sètifikasyon:ISO 10763, DIN 2391, PED 2014/68/EU.

info-300-300

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch