Kabòn Steel soude tiyo ASTM A36 pou livrezon likid presyon ki ba

Pwodwi Deskripsyon
  • Non pwodwi: Astm A36 Steel tiyo
  • Gwosè: Bò (mm): 15*15-500*500,16-273
  • Epesè miray (mm): 1.0-16.0
  • Estanda: ASTM A36
  • Fòm seksyon: rektangilè oswa kare oswa wonn
  • Sifas: Bared, lwil oliv, galvanised, penti vèni, elatriye
  • Kalite: ERW tiyo
  • Longè: 5.8M, 6M, 11.8M, 12M oswa longè Customized. Lòt gwosè yo ka Customized
  • Anbalaj Detay: Estanda ekspòtasyon maritim anbalaj oswa jan sa nesesè.
  • Tan livrezon: 30-50 jou, 7 jou pou machandiz stock.
  • Loading Port: Shanghai, Tianjin, Qingdao.
  • Kapasite Ofri:5 000MT/Pa Mwa.
  • MOQ: 1 Pcs.

ASTM A36 ERW Tiyo Chimik Konpozisyon

Klas C Mn P S Si Kr Mo
A36 Mwens pase oswa egal a 0.26 - Mwens pase oswa egal a 0.04 Mwens pase oswa egal a 0.05 Mwens pase oswa egal a 0.40 - -

ASTM A36 soude tiyo pwopriyete mekanik

Klas

Sede fòs

Fòs rupture

% elongasyon

A36

Pi gran pase oswa egal a 250

400-550

-

A36 Low Carbon Steel Tiyo

erw pipe A36 Welded Pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

GNEE Group se yon manifakti pwofesyonèl ak founisè nan ASTM A36 tiyo asye, A671 tiyo soude, A252 tiyo asye, JIS G3445 ak lòt tiyo soude. Nou kolabore ak moulen asye ki byen koni tankou Angang ak Hegang, epi an menm tan an gen pwòp moulen asye endepandan nou an ki ka satisfè kondisyon Customized ou yo. Achtè soti nan tout mond lan akeyi yo diskite sou òganizasyon ak koperasyon alontèm avèk nou. Si ou bezwen li, ou ka voye nou espesifikasyon espesifik yo epi nou pral site ou pi vit ke posib.