astm a795 vs a53
1. Konparezon Chimik Konpozisyon
| Eleman | ASTM A795 (Gr.B) | ASTM A53 (Klas B) |
|---|---|---|
| Kabòn (C) | Mwens pase oswa egal a 0.26% | Mwens pase oswa egal a 0.30% |
| Manganèz (Mn) | Mwens pase oswa egal a 1.20% | Mwens pase oswa egal a 1.20% |
| Fosfò (P) | Mwens pase oswa egal a 0.05% | Mwens pase oswa egal a 0.035% |
| Souf (S) | Mwens pase oswa egal a 0.05% | Mwens pase oswa egal a 0.035% |
2. Konparezon Pwopriyete Mekanik
| Paramèt | ASTM A795 (Gr.B) | ASTM A53 (Klas B) |
|---|---|---|
| Sede fòs | Pi gran pase oswa egal a 240 MPa | Pi gran pase oswa egal a 240 MPa |
| Fòs rupture | Pi gran pase oswa egal a 415 MPa | Pi gran pase oswa egal a 415 MPa |
| Elongasyon | Pi gran pase oswa egal a 24% | Pi gran pase oswa egal a 24% |
3. Konparezon pèfòmans mekanik
| Karakteristik | ASTM A795 | ASTM A53 |
|---|---|---|
| Egzijans dwat | Mwens pase oswa egal a 0.25% longè | Pa gen okenn kondisyon espesyal |
| Estanda enspeksyon | 100% Weld Enspeksyon | 100% tès idrostatik |
| Ranje Tanperati | -20 degre ~+50 degre | -30 degre ~+80 degre |
4. Diferans aplikasyon
ASTM A795: Sistèm pwoteksyon dife, konduit elektrik sèk, sistèm awozwa machin
ASTM A53: Tiyo transmisyon likid, sipò estriktirèl bilding, fabrikasyon mekanik
A795 soude ak san pwoblèm tiyo asye pou faktori pwoteksyon dife