ASTM A358 EFW tiyo
A358 tiyo asye se yon tiyo elèktrofusion soude austenitic chromium-nikèl alyaj asye pou itilize segondè-tanperati e li se yon estanda spesifikasyon pi sevè pase estanda A312 la.
GNEE Group se yon founisè pwofesyonèl nan Nerjaveèi Elektwo Fusion tiyo ak Tib soude, nou bay yon pakèt pwodwi ki gen ladan 304, 304L, 304H, 309, 309S, 310,310S,316, 316L, 316H,317L,321,321,321,321,321 ,904 ak sou sa. Ou ka kontakte nou nenpòt ki lè si ou bezwen.
A358 EFW Spesifikasyon tiyo
| Estanda |
ASTM, DIN, JIS, GB, AISI, ISO, elatriye lòt estanda entènasyonal yo |
| Dimansyon |
ASTM, ASME, ak API |
| Espesifikasyon |
ASTM A358 / ASME SA 358 - Klas 1, Klas 3, Klas 2, Klas 4, Klas 5 |
| Klas |
TP 304, TP 304L/H, TP 304LN, TP 316L, TP 316, TP 321/H, TP 347/H |
| Gwosè |
8" NB pou 72" NB. |
| Epesè |
3mm a 60mm |
| Longè |
Jiska 6 mèt, longè koupe koutim |
| Epesè miray la |
3mm a 20mm, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S dapre ANSI B36.19/36.10 |
| Fini |
No.1 Pickled Fini, BA Fini, No.4 fini, Electropolished tiyo asye san pwoblèm |
| Kondisyon livrezon |
Fini cho, fini frèt, klere rkwit, rkwit ak marinated, poli, pasivasyon, estrès reviv |
| Aplikasyon |
Endistri manje ak bwason, nikleyè, endistri konstriksyon, tèmik ak plant elektrik, petwochimik, chodyèr, endistri siman, plant jewotèmal, travay enstrimantasyon, travay mekanik, echanjeur chalè, ekipman lwil oliv ak gaz ak travay kanalizasyon. |
| Pake |
Pakèt asye, bouchon plastik nan tou de bout, sache trikote oswa sou demann |
A358 Nerjaveèi asye tiyo konpozisyon chimik
| A358 KLAS |
UNS |
C |
Mn |
P |
S |
Si |
Kr |
Ni |
Mo |
Ti |
Nb |
N |
| TP304 |
S3040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304L |
0.035 |
|
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-13.0 |
|
|
|
|
| TP304H |
S30409 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304N |
S30451 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-18.0 |
|
|
|
0.10-0.16 |
| TP304LN |
S30453 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-12.0 |
|
|
|
0.10-0.16 |
| ASME SA358 TP309S |
S30908 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
0.75 |
|
|
|
| ASME SA358 TP309H |
S30909 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
|
|
|
|
| ASME SA358 TP309Cb |
S30940 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME SA358 TP309HCb |
S30941 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1.10 nmax |
|
| ASME SA358 TP310S |
S3108 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
|
|
| ASME SA358 TP310H |
S3109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
|
|
|
|
| ASME SA358 TP310Cb |
S31040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME SA358 TP310HCb |
S31041 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1.10 max |
|
| ASME A358 TP316 |
S3160 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316L |
S31603 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316H |
S31609 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| TP316Ti |
S31635 |
0.08 |
2.0 |
0.045 |
0.030 |
0.75 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
5x (C-N) -0.70 |
|
0.10 |
| TP316N |
S31651 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| TP316LN |
S31653 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| ASME SA358 TP317 |
S3170 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
10.0-14.0 |
3.0-4.0 |
|
|
|
| ASME SA358 TP317L |
S31703 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
11.0-15.0 |
3.0-4.0 |
|
|
|
| TP321 |
S3210 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP321H |
S32109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP347 |
S3470 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347H |
S34709 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347LN |
S34751 |
0.05-0.02 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
0.20- 50.0 |
0.06-0.10 |
| TP348 |
S3480 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| ASME SA358 TP348H |
S34809 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
ASME SA358 EFW Steel Tiyo Pwopriyete mekanik
| Materyèl |
Chalè |
Tanperati |
Fòs rupture |
Sede fòs |
Elongasyon %, Min |
| Tretman |
Min. |
Ksi (MPa), Min. |
Ksi (MPa), Min. |
| |
º F(º C) |
|
|
| TP304 |
Solisyon |
1900 (1040) |
75(515) |
30(205) |
35 |
| TP304L |
Solisyon |
1900 (1040) |
70(485) |
25(170) |
35 |
| TP316 |
Solisyon |
1900(1040) |
75(515) |
30(205) |
35 |
| TP316L |
Solisyon |
1900(1040) |
70(485) |
25(170) |
35 |
ASTM A358 Steel Tiyo Tolerans
| NPS Designator |
Varyasyon ki otorize nan dyamèt deyò |
| Plis pase Nan. |
Anba Nan. |
| 1/8 jiska 1-1/2, enkli |
1/64 (0.015) |
1/32 (0.031) |
| Plis pase 1-1/2 a 4, enkli |
1/32 (0.031) |
1/32 (0.031) |
| Plis pase 4 a 8, incl |
1/16 (0.062) |
1/32 (0.031) |
| Plis pase 8 a 18, incl |
3/23 (0.093) |
1/32 (0.031) |
Epesè miray nominal
| NPS Designator |
Dyamèt deyò nan. |
Orè 5S nan. |
Orè 10S nan. |
Orè 40S nan. |
Orè 80S nan. |
| 1/4 |
0.540 |
|
0.065 |
0.088 |
0.119 |
| 3/8 |
0.675 |
|
0.065 |
0.091 |
0.126 |
| 1/2 |
0.840 |
0.065 |
0.083 |
0.109 |
0.147 |
| 3/4 |
1.050 |
0.065 |
0.083 |
0.113 |
0.154 |
| 1.0 |
1.315 |
0.065 |
0.109 |
0.133 |
0.179 |
| 1 1/4 |
1.660 |
0.065 |
0.109 |
0.140 |
0.191 |
| 1 1/2 |
1.900 |
0.065 |
0.109 |
0.145 |
0.200 |
| 2 |
2.375 |
0.065 |
0.109 |
0.154 |
0.218 |
| 2 1/2 |
2.875 |
0.083 |
0.120 |
0.203 |
0.276 |
| 3 |
3.500 |
0.083 |
0.120 |
0.216 |
0.300 |
| 3 1/2 |
4.000 |
0.083 |
0.120 |
0.226 |
0.318 |
| 4 |
4.500 |
0.083 |
0.120 |
0.237 |
0.337 |
| 5 |
5.563 |
0.109 |
0.134 |
0.258 |
0.375 |
| 6 |
6.625 |
0.109 |
0.134 |
0.280 |
0.432 |
| 8 |
8.625 |
0.109 |
0.148 |
0.322 |
0.500 |
| 10 |
10.750 |
0.134 |
0.165 |
0.365 |
0.500 |
| 12 |
12.750 |
0.156 |
0.180 |
0.375 |
0.500 |
Mi epesè tolerans ASTM A358 Steel tiyo
| NPS |
ASTM A358 Steel Tiyo Tolerans, % |
| + |
– |
| 1/8-2 1 /2 |
20.0 |
12.5 |
| 3 ~ 18, t/D mwens pase oswa egal a 5% |
22.5 |
12.5 |
| 3~18, t/D> 5% |
15.0 |
12.5 |
| Pi gran pase oswa egal a 20, soude |
17.5 |
12.5 |
| Pi gran pase oswa egal a 20, san pwoblèm, t/D Mwens pase oswa egal a 5% |
22.5 |
12.5 |
| ≥ 20, seamless, t/D> 5% |
15.0 |
12.5 |
GNEE Pwovizyon pou A358 Nerjaveèi asye soude tiyo