ASTM A209 alyaj asye chofaj tib
ASTM A209 ,Specifikasyon Estanda pou Kabòn san pwoblèm-Alyaj Molybdène- Chodyè asye ak Tib Sipèchofaj.
OD: 10mm ~ 203mm
WT: 2.0mm ~ 25mm
Longè: 5.8-12m oswa kòm kliyan yo mande yo
Klas:ASTM A209 T1, ASTM A209 T1a, ASTM A209 T1b
Teknik: San pwoblèm
Itilizasyon:
1. Ba ak mwayen presyon likid transpò tiyo
2. Plant pouvwa
3. Tib chodyè
4. endistri pétrochimique
Pake: lwil oliv tranpe oswa nwa pentire sifas, chaje nan sache navigab, egzagonal fourni.
Konpozisyon chimik:
|
C |
Mn |
P |
S |
Si |
Mo |
|
|
T1 |
0.10-0.20 |
0.30-0.80 |
=0.025 |
=0.025 |
0.10-0.50 |
0.44-0.65 |
|
T1a |
0.15-0.25 |
0.30-0.80 |
=0.025 |
=0.025 |
0.10-0.50 |
0.44-0.65 |
|
T1b |
=0.14 |
0.30-0.80 |
=0.025 |
=0.025 |
0.10-0.50 |
0.44-0.65 |
Pwopriyete mekanik:
|
Klas |
T1 |
T1a |
T1b |
|
Fòs rupture min Ksi (Mpa) |
55(380) |
60(415) |
43(365) |
|
Sede fòs Min Ksi (Mpa) |
30(205 |
32(220) |
28(195) |
|
Elongasyon nan 2in oswa 50mm min% |
30 |
30 |
30 |
Tretman chalè:
Cho fini ak frèt fini tib yo dwe chalè trete nan yon tanperati 650? omwen. Ak plen annaealed, isothermal annealed, oswa nòmalize ak tanperaman kondisyon nan opsyon an nan manifakti a, tanperati a tanperaman minimòm yo dwe pa mwens pase 650 ?.
Tès mekanik obligatwa:
Tès tansyon
Tès plat
Tès dite
Tès elektrik idwostatik oswa nondestructive
| Dyamèt deyò | Longè | Pake estanda |
| OD=168.3mm | L = 13.5m | Bare nan pake ak sèrkl asye (Wonn oswa Egzagonal Fòm) |
13.5mm | Pwoteje anba sèrkl asye (Wonn oswa Egzagonal Fòm) |
|
|
168.3mm | - |
Bare nan ki lach |
|