ASTM A139 vs A252 Steel

1. Konparezon Chimik Konpozisyon

Eleman ASTM A139 ASTM A252 (Gr.3)
Kabòn (C) Mwens pase oswa egal a 0.26% Mwens pase oswa egal a 0.26%
Manganèz (Mn) Mwens pase oswa egal a 1.20% Mwens pase oswa egal a 1.20%
Fosfò (P) Mwens pase oswa egal a 0.05% Mwens pase oswa egal a 0.05%
Souf (S) Mwens pase oswa egal a 0.05% Mwens pase oswa egal a 0.05%
Silisyòm (Si) Mwens pase oswa egal a 0.20% Mwens pase oswa egal a 0.20%

 

2. Konparezon Pwopriyete Mekanik

Paramèt ASTM A139 ASTM A252 (Gr.3)
Sede fòs Pi gran pase oswa egal a 240 MPa Pi gran pase oswa egal a 241 MPa
Fòs rupture Pi gran pase oswa egal a 415 MPa Pi gran pase oswa egal a 455 MPa
Elongasyon Pi gran pase oswa egal a 24% Pi gran pase oswa egal a 20%

 

3. Konparezon pèfòmans mekanik

Karakteristik ASTM A139 ASTM A252
Egzijans dwat Pa gen okenn kondisyon espesyal Mwens pase oswa egal a 0.25% nan longè
Estanda enspeksyon 100% tès idrostatik 100% enspeksyon soude
Ranje Tanperati -30 degre ~+80 degre -20 degre ~+50 degre

 

4. Diferans aplikasyon

ASTM A139‌: Tiyo transmisyon likid, bati sipò estriktirèl, fabrikasyon mekanik

ASTM A252‌: Jeni fondasyon pil, sipò ègzumasyon, estrikti tèminal pò

 