KLAS STEEL ASTM A135 TIYOU SprinKLER

ASTM A135 se yon estanda enpòtan pou elektrik-rezistans-soude tiyo asye. Estanda a kouvri de klas tiyo (Klas A ak Klas B) ki fèt pou transpòte gaz, vapè, dlo, oswa lòt likid. Aspè ki pi enpòtan nan estanda a se egzijans pou kouti soude nan tiyo Klas B yo trete chalè apre yo fin soude oswa trete nan yon fason ke pa gen okenn martensite san tanperaman rete. Egzijans sa a enpòtan anpil pou asire fòs ak rezistans tiyo a. ASTM A135 se jis youn nan anpil estanda ke konpayi yo dwe respekte yo nan lòd yo pwodwi bon jan kalite -tiyo ki pral satisfè bezwen kliyan yo.

DIMANSYON AK GWO ASTM A135 TIYO APROUZE

Yon lis konplè ASTM A135 dimansyon tiyo estanda ki genyen nan ASME B36.10M. ASTM A135 se yon spesifikasyon estanda pou elektrik -rezistans-soude tiyo asye. Li kouvri de klas tiyo asye ERW nan gwosè NPS 2 a 30, ak epesè miray nominal (mwayèn) jiska 12.7mm, enklizif, ak nan gwosè nominal NPS 3/4 a 5 ak yon epesè miray nominal (mwayèn) nan 2.11mm a 3.40mm, tou depann de gwosè. Espesifikasyon sa a kouvri tiyo elektrik-rezistans-soude ki apwopriye pou bride, koube, ak lòt operasyon menm jan fòme, ak pou soude. Rezistans elektrik soude a kalkile lè w divize longè arc la pa zòn seksyon transvèsal la.

 

N.D. O.D. SCH 10 SCH 30/40
Epesè MI PWA NOMINAL Epesè MI PWA NOMINAL
(mm) (pous) (mm) (pous) (mm) (pous) (kg/mèt) (lbs/pye) (mm) (pous) (kg/mèt) (lbs/pye)
15 1/2 21.30 0.84 -- -- -- -- 2.77 0.109 1.27 0.85
20 3/4 26.70 1.05 2.11 0.083 1.28 0.96 2.87 0.113 1.69 1.13
25 1 33.40 1.32 2.77 0.109 2.09 1.41 3.38 0.133 2.5 1.68
32 1-1/4 42.20 1.66 2.77 0.109 2.69 1.81 3.56 0.14 3.39 2.27
40 1-1/2 48.30 1.90 2.77 0.109 3.11 2.09 3.68 0.145 4.05 2.72
50 2 60.30 2.38 2.77 0.109 3.93 2.64 3.91 0.154 5.45 3.66
65 2-1/2 73.00 2.88 3.05 0.12 5.26 3.53 5.16 0.203 8.64 5.8
80 3 88.90 3.50 3.05 0.12 6.46 4.34 5.49 0.216 11.29 7.58
90 3-1/2 101.60 4.00 3.05 0.12 7.41 4.98 5.74 0.226 13.58 9.12
100 4 114.30 4.50 3.05 0.12 8.37 5.62 6.02 0.237 16.09 10.8
125 5 141.30 5.56 3.4 0.134 11.58 7.78 6.55 0.258 21.79 14.63
150 6 168.30 6.63 3.4 0.134 13.85 9.30 7.11 0.28 28.29 18.99
200 8 219.10 8.63 4.78 0.188 25.26 16.96 7.04 0.277 36.82 24.72
250 10 273.10 10.75 4.78 0.188 31.62 21.23 7.08 0.307 51.05 34.27

KONPOZISYON CHIMIK ASTM A135 TIYO

Steel Klas Kabòn max Manganèz Fosfò Souf
Klas A 0.25 0.95 0.035 0.035
Klas B 0.3 1.2 0.035 0.035

PWOPRIYETE MEKANIK ASTM A135 TIYO

ASTM A135 Klas A Klas B

Fòs rupture,

min, ksi [MPa]

48

[330]

60

[415]

Fòs sede,

min, ksi [MPa]

30

[205]

35

[240]

elongasyon,

min, %

35 30

 

OBJEKTIF PETI TIP DIFE ASTM A135 AN WOUJ

Youn nan pati ki pi enpòtan nan yon sistèm sekirite dife se awozwa dife a. Awozwa dife yo fèt pou bay dlo pou siprime oswa etenn yon dife. Anjeneral yo sitiye sou do kay la oswa etaj anwo yo nan yon bilding, ak tiyo ki pote dlo a tipikman pentire wouj pou yo ka fasil vizib nan evènman an nan yon dife. Awozwa dife yo anjeneral aktive pa chalè, epi dlo a egzeyate nan tèt awozwa ki sitiye nan tout bilding lan. Nan pifò ka yo, sèlman awozwa ki pi pre dife a pral aktive, sa ki minimize domaj dlo. Awozwa dife yo se yon pati esansyèl nan nenpòt sistèm sekirite dife, epi itilizasyon yo ka ede sove lavi ak pwopriyete.