EN 10219 Square Hollow Section
Epesè mi: 0.5-20mm
Longè: 0.1 – 18 m, pou chak demann kliyan an
EN 10219 Kare Tib Deskripsyon
EN 10219 tib kare yo se frèt ki fòme oswa ki pa trete chalè soude tib asye kare dapre estanda Ewopeyen an. Itilize nan: konstriksyon, fabrikasyon mekanik, konstriksyon estrikti asye, konstriksyon bato, parantèz jenerasyon pouvwa solè, jeni pouvwa, agrikilti ak machin chimik, mi rido vè, chasi otomobil.
EN 10219 Kare Hollow Seksyon Spesifikasyon
Dyamèt deyò:20 * 20mm - 500 * 500 mm
Epesè mi:0.5-20mm
Longè:0.1 – 18 m, pou chak demann kliyan an
Fen:Koupe kare, Burr retire
Sifas:Lejèman lwil oliv, cho plonje galvanised, Electro galvanised, Nwa
Tretman chalè:Klere rkwit, nwa rkwit


EN 10219 Gwosè seksyon kare kre
| Gwosè mm | kg/m | Gwosè mm | kg/m |
| 20 x 20 x 2.0 | 1.12 | 20 x 20 x 2.5 | 1.35 |
| 25 x 25 x 1.5 | 1.06 | 25 x 25 x 2.0 | 1.43 |
| 25 X 25 X 2.5 | 1.74 | 25 X 25 X 3.0 | 2.04 |
| 30 X 30 X 2.0 | 1.68 | 30 X 30 X 2.5 | 2.14 |
| 30 X 30 X 3.0 | 2.51 | 40 x 40 x 1.5 | 1.81 |
| 40 x 40 x 2.0 | 2.31 | 40 x 40 x 2.5 | 2.92 |
| 40 x 40 x 3.0 | 3.45 | 40 x 40 x 4.0 | 4.46 |
| 40 x 40 x 5.0 | 5.40 | 50 x 50 x 1.5 | 2.28 |
| 50 x 50 x 2.0 | 2.93 | 50 x 50 x 2.5 | 3.71 |
| 50 x 50 x 3.0 | 4.39 | 50 x 50 x 4.0 | 5.72 |
| 50 x 50 x 5.0 | 6.97 | 60 x 60 x 3.0 | 5.34 |
| 60 x 60 x 4.0 | 6.97 | 60 x 60 x 5.0 | 8.54 |
| 60 x 60 x 6.0 | 9.45 | 70 x 70 x 3.0 | 6.28 |
| 70 x 70 x 3.6 | 7.46 | 70 x 70 x 5.0 | 10.11 |
| 70 x 70 x 6.3 | 12.50 | 70 x 70 x 8 | 15.30 |
| 75 x 75 x 3.0 | 7.07 | 80 x 80 x 3.0 | 7.22 |
| 80 x 80 x 3.6 | 8.59 | 80 x 80 x 5.0 | 11.70 |
| 80 x 80 x 6.0 | 13.90 | 90 x 90 x 3.0 | 8.01 |
| 90 x 90 x 3.6 | 9.72 | 90 x 90 x 5.0 | 13.30 |
| 90 x 90 x 6.0 | 15.76 | 90 x 90 x 8.0 | 20.40 |
| 100 x 100 x 3.0 | 8.96 | 100 x 100 x 4.0 | 12.00 |
| 100 x 100 x 5.0 | 14.80 | 100 x 100 x 5.0 | 14.80 |
| 100 x 100 x 6.0 | 16.19 | 100 x 100 x 8.0 | 22.90 |
| 100 x 100 x 10 | 27.90 | 120 x 120 x 5 | 18.00 |
| 120 x 120 x 6.0 | 21.30 | 120 X 120 X 6.3 | 22.30 |
| 120 x 120 x 8.0 | 27.90 | 120 x 120 x 10 | 34.20 |
| 120 X 120 X 12 | 35.8 | 120 X 120 X 12.5 | 41.60 |
| 140 X 140 X 5.0 | 21.10 | 140 X 140 X 6.3 | 26.30 |
| 140 X 140 X 8 | 32.90 | 140 X 140 X 10 | 40.40 |
| 140 X 140 X 12.5 | 49.50 | 150 X 150 X 5.0 | 22.70 |
| 150 X 150 X 6.3 | 28.30 | 150 X 150 X 8.0 | 35.40 |
| 150 X 150 X 10 | 43.60 | 150 X 150 X 12.5 | 53.40 |
| 150 X 150 X 16 | 66.40 | 150 X 150 X 16 | 66.40 |
| 180 X 180 X 5 | 27.40 | 180 X 180 X 6.3 | 34.20 |
| 180 X 180 X 8 | 43.00 | 180 X 180 X 10 | 53.00 |
| 180 X 180 X 12.5 | 65.20 | 180 X 180 X 16 | 81.40 |
| 200 X 200 X 5 | 30.50 | 200 X 200 X 6 | 35.8 |
| 200 x 200 x 6.3 | 38.2 | 200 x 200 x 8 | 48.00 |
| 200 x 200 x 10 | 59.30 | 200 x 200 x 12.5 | 73.00 |
| 200 x 200 x 16 | 91.50 | 250 x 250 x 6.3 | 48.10 |
| 250 x 250 x 8 | 60.50 | 250 x 250 x 10 | 75.00 |
| 250 x 250 x 12.5 | 92.60 | 250 x 250 x 16 | 117.00 |
| 300 x 300 x 6.3 | 57.90 | 300 x 300 x 8 | 73.10 |
| 300 x 300 x 10 | 57.90 | 300 x 300 x 8 | 90.70 |
| 300 x 300 x 12.5 | 112.00 | 300 x 300 x 16 | 142.00 |
| 350 x 350 x 8 | 85.70 | 350 x 350 x 10 | 106.00 |
| 350 x 350 x 12.5 | 132.00 | 350 x 350 x 16 | 167.00 |
| 400 x 400 x 10 | 122.00 | 400 x 400 x 12 | 141.00 |
| 400 x 400 x 12.5mm | 152.00 | 400 x 400 x 16 | 192 |
Gwoup GNEE espesyalize nan fabrikasyon ak founi tib rektangilè EN 10219. Si ou gen nenpòt bezwen oswa ou ta renmen aprann plis, tanpri ou lib pou kontakte nou nenpòt lè.
Baj popilè: en 10219 kare kre seksyon, Lachin en 10219 kare kre seksyon manifaktirè, Swèd
Ou ka renmen tou
Voye rechèch