ASME SA 334 Grade 6 Steel Pipe se yon tiyo asye bendable, fò ak rezistans mete alontèm.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon
Espesifikasyon ASTM A334/A334M kouvri plizyè klas epesè miray minimòm, san pwoblèm ak soude kabòn ak tiyo asye alyaj pou itilize nan anviwònman kriyojenik. Paske epesè miray pi epè ka afekte pwopriyete enpak tanperati ki ba, kèk espesifikasyon pwodwi ka pa konfòme yo ak spesifikasyon sa a.
A334 Gr.6 Kabòn soude tiyo spesifikasyon
| Klas | ASTM A334 Gr.6 Kabòn Steel |
| Gwosè | 1/2" NB pou 36" NB |
| Estanda | ASTM A334, ASME SA334 |
| Gwosè Dyamèt Eksteryè | 1/4"NB Pou 2"NB |
| Epesè miray la | 1 mm a 8 mm |
| Fòm | Wonn, kare, rektangilè, idwolik elatriye |
| Orè | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60% 2c SCH80, SCH120, SCH140, SCH160, XXS |
| Longè | Single Random, Double Random & Koupe Longè. |
| Kalite | Tib san pwoblèm |
| Fen | Plain Fen, Bizote Fen, Treaded |
Konpozisyon chimik nan A334 tiyo
| Eleman | Konpozisyon, % |
| Klas 6yèm A | |
| Kabòn, max | 0.30 |
| Manganèz | 0.29–1.06 |
| Fosfò, max | 0.025 |
| Souf, max | 0.025 |
| Silisyòm | 0.10 min |
| Nikèl | … |
| Kwòm | … |
| Kwiv | … |
| Cobalt | … |
| Molybdène | … |
Pwopriyete mekanik nan A334 Gr.6 ERW tiyo
| Klas 6yèm | ||
| ksi | MPa | |
| Fòs rupture, min | 60 | 415 |
| Fòs Sede, min | 35 | 240 |
| wòch | B 90 | |
| Brinell | 190 | |
Evalyasyon presyon nan A334 soude tiyo ba tanperati
DYAMET DEYÒ |
Epesè MI | PWA TIP NWA | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| GWO NOMINAL PIPE | STANDARD | STANDARD | PLAIN END TIPES | PRESYON TÈS | |||||||
| POUS | MM | POUS | MM | POUS | MM | KG/MTR | MTR/TON | LB/T | FT/TON | PISI | KPA |
| 3/4 | 20 | 1.050 | 26.7 | 0.083* | 2.11 | 1.28 | 781 | 0.86 | 2562 | 700 | 4830 |
| 1 | 25 | 1.315 | 33.4 | 0.109* | 2.77 | 2.09 | 478 | 1.41 | 1568 | 700 | 4830 |
| 1.1/4 | 32 | 1.660 | 42.2 | 0.109* | 2.77 | 2.69 | 372 | 1.81 | 1221 | 1000 | 6890 |
| 1.1/2 | 40 | 1.900 | 48.30 | 0.109* | 2.77 | 3.11 | 322 | 2.09 | 1056 | 1000 | 6890 |
| 2 | 50 | 2.375 | 60.3 | 0.109* | 2.77 | 3.93 | 254 | 2.64 | 833 | 1000 | 6890 |
| 2.1/2 | 65 | 2.875 | 73.0 | 0.120* | 3.05 | 5.26 | 190 | 3.53 | 623 | 1000 | 6890 |
| 3 | 80 | 3.500 | 88.9 | 0.120* | 3.05 | 6.46 | 155 | 4.34 | 509 | 1000 | 6890 |
| 3.1/2 | 90 | 4.000 | 101.6 | 0.120* | 3.05 | 7.41 | 135 | 4.98 | 443 | 1200 | 8270 |
| 4 | 100 | 4.500 | 114.3 | 0.120* | 3.05 | 8.37 | 119 | 5.62 | 390 | 1200 | 8270 |
| 5 | 125 | 5.563 | 141.3 | 0.134* | 3.40 | 11.58 | 86 | 7.78 | 283 | 1200 | 8270 |
| 6 | 150 | 6.625 | 168.3 | 0.134* | 3.40 | 13.85 | 72 | 9.30 | 237 | 1000 | 6890 |
| 8 | 200 | 8.625 | 219.1 | 0.188** | 4.78 | 25.26 | 40 | 16.96 | 130 | 800 | 5520 |
A334 Kabòn Soude Steel Tiyo