API 5L klas X42 ERW liy tiyo
video

API 5L klas X42 ERW liy tiyo

Klas: API 5L X42
Kalite: ERW / soude
Regleman Peman: T/T, L/C
Tan livrezon: 7-25 jou apre yo fin resevwa depo a.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon

API 5L X42 ERW Tiyo Deskripsyon

API 5L X42 welded pipe: API stands for the American Petroleum Institute, with "X" denoting the first letter of "pipeline" in English, capitalized; "42" indicates a minimum yield strength of >420 MPa. Tiyo tiyo X42 se yon tiyo tiyo ak yon klas asye nan X42, prezante pwent plenn, pwent fil, ak pwent priz. Li konekte pa soude, kouple, koneksyon priz, elatriye API 5L X42 soude tiyo yo souvan itilize nan konstriksyon lwil oliv ak gaz natirèl tiyo transmisyon.

PSL-1 Klas:
Tiyo tiyo X42/L290 klas asye: C mwens pase oswa egal a 0.28%, Mn mwens pase oswa egal a 1.30%, P mwens pase oswa egal a {{ 12}}.030%, S mwens pase oswa egal a 0.030%, Nb+V+Ti mwens pase oswa egal a 0.06%, Cu mwens pase oswa egal a 0.50%, Ni mwens pase oswa egal a 0.50%, Cr mwens pase oswa egal a 0.50%, Mo mwens pase oswa egal a 0.15%.

PSL-2 Klas:
Tiyo tiyo L290N/X42N klas asye: C mwens pase oswa egal a 0.24%, Mn mwens pase oswa egal a 1.20%, P mwens pase oswa egal a {{ {10}}.025%, S mwens pase oswa egal a 0.015%, Nb mwens pase oswa egal a {{2{{22 }}}}.05%, V mwens pase oswa egal a 0.06%, Ti mwens pase oswa egal a 0.04%, Cu mwens pase oswa egal a 0.50%, Ni mwens pase oswa egal a 0.30%, Cr Mwens pase oswa egal a 0.30%, Mo mwens pase oswa egal a 0.15%, B Mwens pase oswa egal a 0.004%.

Tiyo tiyo L290M/X42M klas: C mwens pase oswa egal a 0.22%, Mn mwens pase oswa egal a 1.30%, P mwens pase oswa egal a {{ 10}}.025%, S mwens pase oswa egal a 0.015%, Nb mwens pase oswa egal a {{2{{22} }}}.05%, V mwens pase oswa egal a 0.05%, Ti mwens pase oswa egal a 0.04%, Cu mwens pase oswa egal a 0.50%, Ni mwens pase oswa egal a 0.30%, Cr mwens pase oswa egal a 0.30%, Mo mwens pase oswa egal a 0.15%, B Mwens pase oswa egal a 0.004%.

API 5L estanda X42/L290 kondisyon tès tansyon materyèl:
PSL-1 Klas: Sede fòs ki pi gran pase oswa egal a 290MPa, fòs Tensile ki pi gran pase oswa egal a 415MPa.

PSL {{0}} Klas: Sede Fòs 290MPa ~ 495MPa, Fòs Tensile: 415MPa ~ 655MPa, Sede ak Pwopòsyon Tensile Mwens pase oswa egal a 0.93.

API 5L X42 ERW Tib Spesifikasyon

Klas X42 / L290 (N, M, Q, R)
X42 PSL1: 1.0483
X42 PSL2: 1.0484
Estanda API 5L
O.D. 16" pou 54"
Fen tiyo

Buttweld, Vibrateur Manje, Bizote Fen (BE), Koupe Grooves, Plain fen (PE), Vise, Flanged Fen, Grooved, Socket, Chanfreinage, Threaded Fen (Gason ak Fi), Koupe Fil

Epesè miray la SCH160, SCH40, SCH-XXS, SCH-XS, SCH-STD, SCH80,

API 5L X42 ERW Steel tiyo

x42 line pipex42 erw steel tubing

Baj popilè: api 5l klas x42 erw liy tiyo, Lachin api 5l klas x42 erw liy tiyo manifaktirè, Swèd