Pre-galvanize, konnen tou kòm galvanising moulen, enplike nan pase fèy asye nan zenk fonn. Apre pwosesis sa a, fèy asye a koupe nan gwosè a vle ak re-woule. Pandan pre-galvanising, tout fèy asye a kouvwi ak yon epesè espesifik nan zenk. Pou egzanp, fèy asye Z275 pre-galvanize gen yon epesè kouch zenk nan 275 gram pou chak mèt kare.

Pwodwi: tiyo galvanised, tiyo asye galvanised, tiyo asye pre galvanised, tiyo asye pre-galvanize
Aplikasyon: Itilize pou transpòte likid presyon ba, gaz ak chofaj.
Gwosè: OD: 21.3mm ~ 610mm
WT: 0.5mm ~ 20mm
LONGÈ: 0.3mtr ~ 18mtr, Ramdon Length, Fixed Length, SRL, DRL
Estanda GB/T 3091 Q195/Q215/Q235/Q345, BS 1387, EN 39, EN 1139 S235JR/S275JR, ASTM A53 GR. A/B/C, JIS G3444 STK 400/STK 500

 

 

 

 

 

 

 

 

 

 

Spesifikasyon

PWODWI

Epesè (MM)

LONGÈ

ESTANDA

Tiyo galvanize

jiska 9mm

Longè o aza nan 4 a 7 mèt sof si espesifye otreman

IS : 1239 [PART1] / 1990

ERW KONSTRUKSYON TIYO ACYE GALVANIZE CHO-PLONGE

DYAMET EXTERNO

(D)

Epesè MI (yo) mm

PWA kg/m

Φ

pous

manm

1.80

2.00

2.30

2.50

3.00

3.20

3.60

4.00

Φ21

1/2"

21.3

0.87

0.95

1.08

1.16

1.35

1.43

1.57

1.71

Φ26

3/4"

26.9

1.11

1.23

1.40

1.50

1.77

1.87

2.07

2.26

Φ33

1"

33.7

1.42

1.56

1.78

1.92

2.27

2.41

2.67

2.93

Φ42

1 1/4"

42.4

1.80

1.99

2.27

2.46

2.91

3.09

3.44

3.79

Φ48

1 1/2"

48.3

2.06

2.28

2.61

2.82

3.35

3.56

3.97

4.37

Φ60

2"

60.3

2.60

2.88

3.29

3.56

4.24

4.51

5.03

5.55

Φ76

2 1/2"

76.1

3.30

3.65

4,19

4.54

5.41

5.75

6.44

7.11

Φ88

3"

88.9

3.87

4.29

4.90

5.33

6.36

6.76

7.57

8.37

Φ114

4"

114.3

4.98

5.54

6.34

6.89

8.23

8.77

9.83

10.88